Complex Board Design Induced Solder Separation Failure



Complex Board Design Induced Solder Separation Failure
The study elaborates the parameters with the solder separation failure per board design configuration, and also provides the potential solution to mitigate the failure. An in-depth analysis on the solder joint microstructure utilizing Electron-backscattered diffraction (EBSD) supports the test results leading to the mechanism associated with the solder separation failure.
Technical Paper

DOWNLOAD

Authored By:


Tae-Kyu Lee, Gnyaneshwar Ramakrishna
Cisco Systems
CA, USA

Jonghyun Nam, Daljin Yoon, and Heera Roh
SK Hynix
Icheon, Korea

Summary


The increase of functionality and performance in electronic systems and devices induce more complex printed circuit board design features with more Cu layer counts, increased thickness, and with a demand for less impact to the high-speed signals. These combinations drive the PCB design to configurations including via-in pad platted over (VIPPO) with back-drill process, which resulted in a mixture of various stress distributions in a given printed circuit board.

Recent studies revealed that these mixed design features can induce failure during a second reflow at the solder joint interface known as solder separation. Through a series of in-situ resistance measurements during reflow, the accurate separation location and temperature are identified per design configuration and solder joint material combination. A 10x15mm BGA component with 10x20 array solder balls were assembled on 28 Cu-layered 140mil thickness boards, which contain a mixture of VIPPO and VIPPO+back-drilled pads compared to a full VIPPO pad design as a baseline.

The assembled boards were subject to in-situ resistance measurements during second reflow. The segmented daisy chains per component allowed the detection of solder separation during reflow at the exact solder joint location, which are associated with the failure symptoms. The failure signature was detected at 210-212oC during heating cycle at solder joint locations, which are adjacent to solder joints with higher z-axis expansion, in this case full VIPPO location adjacent to back-drilled VIPPO pad locations. Three different solder alloys were selected to investigate the sensitivity to solder separation defects along with the evaluation per long-term thermal cycling performance.

The results indicated that the separation defect in SAC305 can be mitigated by using SAC305+SnBiAg low melting temperature (LTS) hybrid solder joint configuration and full LTS configuration. The presented study elaborates the parameters associated with the solder separation failure per board design configuration, and provides the potential solution to mitigate the failure. An in-depth analysis on the solder joint microstructure utilizing Electron-backscattered diffraction (EBSD) supports the test results leading to the mechanism associated with the solder separation defect failure.

Conclusions


Through a series of in-situ resistance measurement during second reflow, the accurate separation time and temperature are identified per design configuration and solder joint alloy material combination. The solder separation defect induced failures detected at 210-212oC at full VIPPO solder joint locations, which are adjacent to solder joints with higher z-axis expansion, in this case, back-drilled VIPPO and dog-bone/floating pad locations. Three different solder alloys were selected to investigate the sensitivity to solder separation defects along with the evaluation per long-term thermal cycling performance.

The results indicated that the separation defect in second reflowed SAC305 joints can be mitigated with using the SAC305+SnBiAg hybrid solder joint configuration and full LTS configuration since it has lower than 212oC assembly peak temperature. Thermal cycling performance after second reflow also shows the hybrid LTS is not affected by the uneven VIPPO distribution induced stress conditions. The presented study elaborates the parameters associated with the solder separation failure per board design configuration, and also provides the potential solution to mitigate the failure. An in-depth analysis on the solder joint microstructure utilizing Electron-backscattered diffraction (EBSD) supports the test results leading to the mechanism associated with the solder separation failure.

Comments

No comments have been submitted to date.

Submit A Comment


Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Advanced-Interconnections

Need Improved Solder Joint Visibility?
Solder Peel-A-Wayš Removable Terminal Carriers in place and peel the carrier away for complete solder joint visibility on both sides of the PCB. Watch a video to see it in action.
Advanced Interconnections Corp.