circuitnet
Sponsor
Advanced Interconnections Corp.
Plan Ahead for BGA Device Upgrades
BGA Socket Adapter Systems convert surface mount device packages to through-hole (pinned) assemblies, making it easy to plug and unplug SMT devices in the field or the test lab.
Advanced Interconnections Corp.
Rentals and Rent to Purchase x-ray Systems
Sponsor
ECD
Maybe it's the thermocouple connection
If your thermal profiling readings seem inconsistent, the culprit could be your thermocouple attachment method. A recently conducted study revealed some interesting findings.
ECD
Viewpoint
January 28, 2013

Shen Hwang Ting, Global Marketing Manager, CyberOptics

For several years companies around the United States have been on-shoring jobs that were previously sent overseas. Companies who have off-shored in the past have experienced quality problems, communication issues, intellectual property issues and increasing shipping costs.




The White House has promised to provide incentives for businesses to bring jobs back from China, Japan and Mexico to the United States. These are some good reasons to see an increase of US manufacturing jobs in the coming year.




Apple, Google and GE have already announced plans to bring manufacturing jobs back to the US in 2013. These may seem like a drop in the bucket but it is an ongoing trend. With these new US jobs there will be a need for capital equipment as well as hand tools which is where our products fit into the picture.



Our plan for 2013 includes continuing to search out new customers and distribution through trade show attendance, print marketing and an increased online presence. We will continue to promote our product line as safe hand-tools for manual-handling of micro-sized as well as larger parts in critical-environment manufacturing processes. We expect to see stronger sales in 2013 and will add staff as increased sales dictates.

Shen Hwang Ting
Global Marketing Manager, CyberOptics (Singapore) Pte. Ltd.
Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling