circuitnet
Sponsor
Advanced Interconnections Corp.
Plan Ahead for BGA Device Upgrades
BGA Socket Adapter Systems convert surface mount device packages to through-hole (pinned) assemblies, making it easy to plug and unplug SMT devices in the field or the test lab.
Advanced Interconnections Corp.
Rentals and Rent to Purchase x-ray Systems
Sponsor
ECD
Maybe it's the thermocouple connection
If your thermal profiling readings seem inconsistent, the culprit could be your thermocouple attachment method. A recently conducted study revealed some interesting findings.
ECD

Solid-State Diffusion between Rolled Cu and Electroplated Matte-Sn System



Solid-State Diffusion between Rolled Cu and Electroplated Matte-Sn System
This study focusses on the IMC phase growth in rolled Cu- electroplated Sn system during the temperature range from 398K to 473K.

DOWNLOAD
Authored By:
Abhilaash Ajith Kumar, Werner Hügel, Ph.D.
Robert Bosch GmbH
Schwieberdingen, Germany

Summary

Ever increasing need for miniaturization and high-density electronics, leads to higher intermetallic (IMC) phase/solder ratio affecting the ductility of the solder joint. The diffusion behavior and growth of intermetallic (IMC) phases of Cu-Sn system is studied through isothermal aging over wide range of temperature from 398K to 473K. Cu-Sn binary couples, prepared by electroplating Sn over bulk Cu, are aged at 398K, 423K, 453K and 473K for various times to investigate the microstructural development and growth kinetics of the IMC phases.

In-house developed algorithm was used to detect and quantify the Cu6Sn5 and Cu3Sn morphology from electron microscopy images. Considering the narrow compositional range and interdependent growth/dissolution of the two IMC phases, Wagner’s method is used to evaluate the integrated interdiffusion coefficients based on the measured IMC thicknesses. The activation energies and the diffusion constants of the Cu6Sn5 and Cu3Sn IMC phases have been calculated from the integrated interdiffusion coefficients.

Conclusions

The following conclusions are obtained from this work regarding the solid-state diffusion in rolled Cu – electroplated Sn system.
  • Microstructural investigation revealed the presence of cracks along the grain boundaries of Cu6Sn5 and at the interface between Cu3Sn|Cu6Sn5 at both low and high temperatures after isothermal aging. This can lead to early failure of the solder joint.
  • Integrated interdiffusion coefficients and activation energies for Cu6Sn5 and Cu3Sn have been calculated in this study.
  • The lower activation energies of Cu6Sn5 and Cu3Sn confirms grain boundary diffusion growth of IMC phases between 398K – 473K.
  • Fine grains in rolled Cu substrate enhances relatively the growth of Cu3Sn and results in overall lower total IMC thickness at the interface between Cu and Sn.

Initially Published in the SMTA Proceedings
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling