circuitnet
Sponsor
Advanced Interconnections Corp.
Plan Ahead for BGA Device Upgrades
BGA Socket Adapter Systems convert surface mount device packages to through-hole (pinned) assemblies, making it easy to plug and unplug SMT devices in the field or the test lab.
Advanced Interconnections Corp.
Rentals and Rent to Purchase x-ray Systems
Sponsor
ECD
Maybe it's the thermocouple connection
If your thermal profiling readings seem inconsistent, the culprit could be your thermocouple attachment method. A recently conducted study revealed some interesting findings.
ECD

Ball Pull Test Efficiency for the PCB Pad Cratering Validation



Ball Pull Test Efficiency for the PCB Pad Cratering Validation
In the study cold ball pull testing is used to validate the resistance of PCB pad cratering for different ultra-low loss dielectrics materials.

DOWNLOAD
Authored By:
Jeffrey ChangBing, LeeCheng-Chih Chen, Alice Lin, Dem Lee
iST- Integrated Service Technology, Inc., TAIWAN
Gary Long, Consultant, USA
Masahiro Tsuriya, INEMI, JAPAN

Summary

Cold ball pull testing is used to validate the resistance of PCB pad cratering for the different ultra-low loss dielectrics materials (Dk=3~4.2 and Df <= 0.005 @ 1GHz) in the study. The materials were fabricated in multiple PCB shops using a common test board design utilizing a coupon to result in a 16 mil nominal pad size for the pulls. After fabrication, a 20 mil SAC305 ball is SMT attached to the 16 mil nominal pads for pulling.

Each material had 3 coupons with 50 pull locations on each to generate 150 data points for statistical analysis. The peak pull force differences of the material builds can be compared to differentiate the results. As a result, the different ultra-low loss dielectric material's performance to withstand PCB pad cratering can be compared comprehensively with the cold ball pull test.

Conclusions

Cold ball pull testing allows PCB shops to compare which dielectric materials have the best performance to withstand pad cratering based on their process control so as to reduce the field return rate due to pad cratering in PCB assembly and in service life. The comparison of data from different PCB shops is still not suggested due to process deviations at the different shops.

The test method was demonstrated to be reproducible when carefully executed and produced no anomalous results, suggesting it is a good practical test. It was not concluded that the material with certain cold ball pull strength will be capable of withstanding actual PCB pad cratering during shipping and service life of product, but was able to provide differentiation between materials at a single fabricator, thus allowing the end user to select the best candidate material for that PCB shop. The next steps will be to determine peak pull force thresholds at which pad cratering happens when materials are used in real service. Relating this work to results of other methods, such as impact testing, spherical bend testing, DMA, etc. is recommended to accomplish that task. Thresholds are expected to be different depending on product design and fabricator process control.

Initially Published in the IPC Proceedings
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling