Jetting Solder Paste Opens Up New Possibilities



Jetting Solder Paste Opens Up New Possibilities
The differences between jet printing and dispensing will be highlighted and technical challenges with broad band technology will be discussed.

DOWNLOAD
Authored By:
Nico Coenen
MYDATA
Taby, Sweden

Summary

Jetting of liquids is becoming the standard in our industry. MYDATA has developed a unique tool to jet solder paste. This non-contact method of applying solder paste has a large number of advantages compared to standard screen printing or dispensing.

The challenges of today's production environment is not only the fact that components getting smaller but the biggest challenge is the combination of small and large components on the same board. Putting the right amount of solder paste for each component will be required to deliver the right quality. Depending on the volume requirements Jet Printing can be an alternative tool to cope with this mix or be used as an add on tool to compliment the screen printer in a high volume environment.

The Jet Printing technology allows to build up the volume by single dots to achieve the right amount for each component. Special applications like pin in paste, applying paste in cavities and many more challenges of today's requirement can be easily accommodated with this technology.

Mixing different types of solder paste with different metal content will be discussed as typically jet printing paste is type 5 versus type 3 or 4 for a screen printer. The differences between jet printing en dispensing will be highlighted and technical challenges with broad band technology will be discussed.

Conclusions

Over the years jetting has gained importance and has become the standard in the industry to apply fluids. A non- contact way has many advantages over a traditional dispensing process. Jet Printing of solder paste can be used in low to mid volume segments to replace a screen printer but can also be added in high volume lines to take care of the challenging deposits or to add solder paste where needed.

Today Jet Printing is no longer seen as a futuristic technology but it has proven itself and the technology is still gaining momentum. With all the developments going on it looks like Jet Printing will increase further the coming years.

Initially Published in the SMTA Proceedings
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling