3D IC Integration Technology Development in China



3D IC Integration Technology Development in China
China's semiconductor foundry and microelectronic packaging industries are embracing the move to join 3D IC integration.

DOWNLOAD
Authored By:
Wei Koh, Ph.D.
Pacrim Technology
Irvine, CA, USA

Summary

China's semiconductor foundry and microelectronic packaging industries are embracing the move to join 3D IC integration technology development with ample funding and rapid pace. An overview of the recent progress on the efforts in 3D IC integration technology development by the leading domestic companies and research institutes is provided here.

Because China still lacks in infrastructure for advanced and modern front end of the line (FEOL), backend of the line(BEOL), and middle-end of the line (MEOL) process capabilities for 300mm wafers, development efforts on 3D IC integration have many limitations to begin with. The efforts adopted by some leading research institutes and back-end packaging assembly and test companies; however, appear to be quite ingenuous and pragmatic, by selecting more easier "cutting-in" research projects and processes that require less initial capital investment and infrastructural establishments.

The pattern of latest development efforts can be divided into two major areas: 1) TSV materials, processing, and interconnection; 2) low-cost interposer and 2.5D integration assembly application in wafer level CSP packages for MEMS and sensors using small-sized wafers. The short term perspectives and longer term growth opportunities for China's indigenous development efforts on 3D IC integration is summarized in conclusion.

Conclusions

A multi-pronged progress in 3D IC integration research has been made by several leading research institutes and companies such as Huawei and JCAP within just a few years. Many applications are aimed at using 4 and 6-in size wafers, where wafer thinning, bonding and TSV fabrication are relatively easier compared to that for 300mm wafers. The near term fruit and resulting strength in China's efforts will be in practical, low-cost applications for camera modules, sensors, and MEMS.

Some companies (Huawei, SMIC) are also planning to move into more complex interposers and 2.5D integration applications. In China, there are still plenty of market opportunities and growth potentials for mobile and computing devices to adopt 3D IC integration technologies for eventual high volume manufacturing in the coming years.

Initially Published in the SMTA Proceedings
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling