Maybe it's the thermocouple connection
If your thermal profiling readings seem inconsistent, the culprit could be your thermocouple attachment method. A recently conducted study revealed some interesting findings.
ECD

Quantitative Analysis of Corrosion Resistance



Quantitative Analysis of Corrosion Resistance
An electrochemical method via sequential electrochemical reduction analysis instrument to quantify the corrosion resistance of the EN deposit is proposed.

DOWNLOAD
Authored By:
Dr. Lei Jin, Dr. Jun Nable, Dr. Kesheng Feng, Lenora Toscano, Dr. Ernie Long
Electronics Solutions, MacDermid, Inc.
Waterbury, CT USA

Summary

An electroless nickel (EN) layer is frequently used in various industrial applications. Commonly it is used as the barrier layer in electroless nickel/immersion gold (ENIG) as a solderability preservative for the electronics industry. The finish provides excellent corrosion resistance and good solderability. A shortcoming of this process is the potential for a hyperactive corrosion of the nickel surface during immersion gold plating. The resultant defect displays itself as a gray or black appearance at the nickel/gold interface, known as "Black Pad" or "Black Line Nickel".

It is important to determine and control the corrosion properties of an EN deposit during an ENIG process to obtain high quality products. Unfortunately, quantitative analysis of corrosion resistance of the EN layer has not been established in the field of PCB. In this paper, an electrochemical method via sequential electrochemical reduction analysis (SERA) instrument to quantify the corrosion resistance of the EN deposit is proposed. The data obtained via the electrochemical method was analyzed and correlated to the deposit properties of the EN. The method is easy to use and can be applied for quantitative analysis in industrial EN processes.

Conclusions

Results presented here show that the new SERA test method can be applied on a routine basis to assess the corrosion resistance behavior of EN deposit. This method is a relatively simple, fast, and quantitative analysis. Within the same EN bath, this method can even be used to determine P% at different points on a PCB boards. This proposed method can also been applied on other applications, such as EN quality control, product screening, and formulation comparisons on a simple and quantitative basis.

Initially Published in the IPC Proceedings
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling