Reliability of Low Silver, Lead-Free Joints



Reliability of Low Silver, Lead-Free Joints
The objective of this study is to assess the reliability under loading conditions of low silver solder solder pastes.

DOWNLOAD
Authored By:
Vikram Srinivas, Nicholas Williard, Preeti Chauhan and Michael Osterman
Center for Advanced Life Cycle Engineering
Department of Mechanical Engineering
University of Maryland
College Park, MD, USA

Summary

To improve the durability of lead free solder joints under high strain rates, such as drop and shock loading, some area array manufacturers have converted to low silver (Ag) content tin silver copper (SAC) solder spheres instead of the commonly accepted SAC305 solder. While the lower silver content SAC solder joints may address high strain rate shock loads, the durability of these joints under low strain rates has to be taken into consideration.

The objective of this study is to assess the reliability under loading conditions with strain rates several orders of magnitude below that observed in drop testing. To this end, thermo-mechanical loading induced by temperature cycling (-55°C to 125°C) and mechanical loading induced by cyclic board level mechanical torsion were considered. Test vehicles were assembled using SAC305 solder paste with eight peripheral ball grid array packages (BGA) per printed wiring board with SAC105, SAC125Ni and SAC305 solder spheres.

Four test specimens per type were assembled. Two of test specimens of each solder combination were then subjected to temperature cycling, while the remaining two were subjected to mechanical torsion. In-situ electrical resistance monitoring was performed on the low electrical resistance paths formed by the individual packages and the printed wiring board. Statistical analysis was conducted on cycles to failure data collected from the defined tests. A drop in fatigue durability with decrease in silver content in the solder spheres was observed for both thermo-mechanical and mechanical loading.

Conclusions

Under temperature cycle test, durability was observed to drop with a reduction in silver (Ag) content i.e. SAC305 (96.5%Sn + 3.0%Ag + 0.5%Cu)> SAC125Ni (98.25%Sn + 1.2%Ag + 0.5%Cu+0.05%Ni) > SAC105 (98.5%Sn + 1.0%Ag + 0.5Cu Under mechanical torsion cycling, durability of tested solders was observed to follow the same trend. SAC305 solder joints exhibits higher characteristic life in both type A and B configurations compared to mixed reduced-Ag SAC solders such as SAC125 and SAC105 at lower strain rates when compared to drop test results in literature.

Initially Published in the SMTA Proceedings
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling