Maybe it's the thermocouple connection
If your thermal profiling readings seem inconsistent, the culprit could be your thermocouple attachment method. A recently conducted study revealed some interesting findings.
ECD

Weight Limit for Double Sided Reflow of QFNs



Weight Limit for Double Sided Reflow of QFNs
Study determines the maximum weight of a QFN on a circuit board by SAC305 solder surface tension when the board was upside down in a reflow oven.

DOWNLOAD
Authored By:
Sasha Smith, David Connell and Bev Christian
Research In Motion
Waterloo, ON, Canada

Summary

QFNs of two different sizes with different weights attached to them were used to determine the maximum potential weight of a QFN that could be held on a printed circuit board by SAC305 solder surface tension alone when the board was upside down in a reflow oven. Different pad geometries were used and the effect of voiding was also taken into consideration.

Conclusions

A constant of approximately 0.0269 g/mm represented the ratio at which a molten SAC305 solder joints failed to hold a QFN on the bottom side of a PCB during reflow, as a function of component mass versus total perimeter of wetted surface. Applying a 20% failure buffer to this value produced an average failure ratio of 0.0215. The standard deviation associated with this value was very small
indicating minimal variance and most likely well suited to applications that involve many different component types.

Certainly for QFN 2 taking into account void perimeter resulted in a tighter grouping of the failures.
QFN components with a greater surface area demonstrated a higher level of variance for the percentage failure as a function of the component weight versus total wetted perimeter ratio. A recommendation would be to custom make added weights so they cover the entire surface of the part to be tested. This would result in less chance of not having the weight centered and it would provide less surface
area to be affected by oven air turbulence. Monolithic weight would also mostly eliminate different amounts of glue sued to hold multiple weights to the parts being tested.

The range of components tested should be expanded. A wider range of components should be tested to verify whether or not it would be appropriate to the apply the ratio determined from this experiment to various other components involved in the manufacturing process.

All work should be duplicated in batch and conveyorized ovens to see if there is a major difference due to oven type. Reduce the number of runs for each test board. Board stress such as blistering and warping was observed on boards that had been tested more than three times. While boards were only tested a maximum of three times with no visible stress, internal stress may have occurred after the first run. Fewer runs for each board should be done to determine if this will have an effect on the consistency of results.

Initially Published in the SMTA Proceedings
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Uyemura
RAIG Minimizes Corrosion, Allows Higher Gold on ENEPIG
Paper describes a mixed reaction RAIG electrolyte that minimizes galvanic corrosion and allows higher ENEPIG gold thicknesses, enabling robust designs and world-class quality on target with minimal variation.
Uyemura
Affordable Profiling