Reliability of New SAC-Bi Solder Alloys in Thermal Cycling with Aging



Reliability of New SAC-Bi Solder Alloys in Thermal Cycling with Aging
The effect of micro-alloying to SAC based solder materials on component reliability was studied, considering various factors of solder paste and surface finish.
Technical Paper

DOWNLOAD

Authored By:


Francy John Akkara, Mohammed Abueed, Mohamed Belhadi, Xin Wei, Dr. Sa’d Hamasha, Dr. Haneen Ali
NSF Center for Advanced Vehicle and Extreme Environment Electronics (CAVE3)
Department of Industrial and Systems Engineering

Dr. Jeff Suhling, Dr. Pradeep Lall
Department of Mechanical Engineering
Auburn University, Auburn AL 36849

Summary


Drive towards lead-free electronics began in the early 2000s. Solder pastes based on tin (Sn), copper (Cu), and silver (Ag) were the initial replacement for the traditional SnPb solder. With the SAC alloys, several researches reported that one year of aging consumed more than 50% of the component life. Once the detrimental effects of aging were discovered, the industry started the search for better solder paste materials. The SAC based pastes were made better by adding elements such as Bismuth (Bi), Antimony (Sb), Nickel (Ni). Recently, all the leading manufacturers have introduced new solder materials that claim to have high reliability in harsh environments. Extensive tests are required to filter the best solder pastes. In the study, three high reliability solder materials from leading manufacturers have been selected and used for the test vehicle assembly. SAC305 paste is also included for comparison with the new materials. The test vehicle is a printed circuit board (PCB) of FR-4 laminate material with three CABGA208s (15x15mm) with SAC305 spheres, three LGA36s, and six SM resistors. Three surface finishes, namely electroless Nickel immersion Gold (ENIG), immersion Silver (ImAg), and organic solderability preserve (OSP), have been considered for the study. Immediately after assembly, all boards are aged for a period of twelve months at 125oC. All the boards are then thermally cycled for 5000 cycles from -40oC to +125oC with a ramp time of 50 minutes and dwell times of 15 minutes at high and low temperatures.

Two parameters Weibull analysis is used to quantify the performance of the different alloy materials. ANOVA analysis involving the different composition and surface finish is also done in order to get insight into the most influential factors on the component reliability. Generally, all the new alloys were found to outperform SAC305 paste. Materials with a high content of Bi, Sb, and Ag performed the best in the lot. The microstructure analysis showed that bulk solder failure was the typical failure mode with the crack propagating in bulk along with the intermetallic compound layer on the component side.

Conclusions


In this paper, the effect of micro-alloying different elements to SAC based solder materials on component reliability was studied using 15mm x 15mm CABGA, considering various factors of solder paste and surface finish. For each surface finish, the alloys involved in the study were analyzed. It was observed that the new elements have positively contributed to the component reliability. The micro-alloyed solder pastes proved to be more reliable than SAC305 alloy. Adding elements such as Bi, Sb, Ni, and Co to the SnAgCu solder joint was found to improve the fatigue resistance and slows down the adverse effect of aging and thermal cycling on the component reliability.

Initially Published in the SMTA Proceedings

Comments

No comments have been submitted to date.

Submit A Comment


Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Viscom-SE

iX7059 Series by Viscom: Inline X-ray Inspection Power
High-performance Inline X-ray Inspection Systems for complex electronics, semiconductors, and power modules up to 200 kg. Seamless integration, AI-powered accuracy, and maximum reliability for every application.
Viscom SE