Epoxy Offers Ultra High Heat Transfer
Bond EP5TC-80 is a NASA low outgassing rated epoxy that achieves a thermal conductivity of 3.3-3.7 W/(m·K), while also retaining its electrical non-conductivity.
Master Bond
|
|
Low Temperature SMT Solder Evaluation
Recent advances in alloy "doping" have opened the door to revisit Sn/Bi alloys as a possible alternative to SAC-305 for many applications.
Technical Paper
DOWNLOAD
|
Authored By:
Howard "Rusty" Osgood, David Geiger, Robert Pennings, Christian Biederman, Jie Jiang, Jon Bernal
Flextronics International
Milpitas, CA, USA
Summary
The electronics industry could benefit greatly from using a reliable, manufacturable, reduced temperature, SMT solder material (alloy-composition) which is cost competitive with traditional Sn3Ag0.5Cu (SAC305) solder. The many possible advantages and some disadvantages / challenges are discussed.
Until recently, the use of Sn/Bi based materials has been investigated with negative consequences for high strain rate (drop-shock) applications and thus, these alloys have been avoided. Recent advances in alloy "doping" have opened the door to revisit Sn/Bi alloys as a possible alternative to SAC-305 for many applications.
We tested the manufacturability and reliability of three low-temperature and one SAC-305 (used as a control) solder paste materials. Two of these materials are doped Sn/Bi/Ag and one is just Sn/Bi/Ag1%.
We will discuss the tests and related results. And lastly, we will discuss the prospects, applications and possible implications (based on this evaluation) of these materials together with future actions.
Conclusions
Preliminary results investigating the low temperature paste alloys against the Sn3Ag0.5Cu paste alloy look promising. Limited internal testing to date, combined with limited external testing data, indicates that these newer, doped, lower temperature solders perform as well or better than Sn3AgCu(SAC305).
Further testing and evaluation is needed and is underway. We are proceeding with drop/shock and higher strain rate monotonic bend testing which is where we expect to see differentiation between the doped and non-doped solders under investigation.
Initially Published in the SMTA Proceedings
|
Comments
|
No comments have been submitted to date.
|
|
|
|
Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.
Insert Your Email Address
|
| Sponsor |
|
Built to Scale. Proven in Production.
Microsystems World CNC boosted throughput and automation by trading up to a complete inline SMT solution—powered by Manncorp and designed for long-term growth.
Manncorp Inc.
|
|
|