| Sponsor |
|
Epoxy Offers Ultra High Heat Transfer
Bond EP5TC-80 is a NASA low outgassing rated epoxy that achieves a thermal conductivity of 3.3-3.7 W/(m·K), while also retaining its electrical non-conductivity.
Master Bond
|
|
High-Speed 3D Surface Imaging Technology in Electronics Manufacturing
This paper introduces line confocal technology that was developed to characterize 3D features of surface and material types at sub-micron resolution.
Technical Paper
DOWNLOAD
|
Authored By:
Juha Saily, FocalSpec, Inc., Santa Clara, CA, USA
Summary
This paper introduces line confocal technology that was recently developed to characterize 3D features of various surface and material types at sub-micron resolution. It enables automatic microtopographic 3D imaging of challenging objects that are difficult or impossible to scan with traditional methods, such as machine vision or laser triangulation. Examples of well-suited applications for line confocal technology include glossy, mirror-like, transparent and multi-layered surfaces made of metals (connector pins, conductor traces, solder bumps etc.), polymers (adhesives, enclosures, coatings, etc.), ceramics (components, substrates, etc.) and glass (display panels, etc.). Line confocal sensors operate at high speed and can be used to scan fast-moving surfaces in real-time as well as stationary product samples in the laboratory. The operational principle of the line confocal method and its strengths and limitations are discussed. Three metrology applications for the technology in electronics product manufacturing are examined: 1. 3D imaging of etched PCBs for micro-etched copper surface roughness and cross-sectional profile and width of etched traces/pads. 2. Thickness, width and surface roughness measurement of conductive ink features and substrates in printed electronics applications. 3. 3D imaging of adhesive dots and lines for shape, dimensions and volume in PCB and product assembly applications.
Initially Published in the SMTA Proceedings
|
Comments
|
No comments have been submitted to date.
|
|
|
|
Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.
Insert Your Email Address
|
| Sponsor |
|
Reflow Solderable TIM1 Thermal Grease
AIT's CGR7016 & CGR7019-LB series are proven reliable for thermal interface usage at extreme temperatures. 100% chip to heat-spreader lid seal after multiple reflow soldering.
AI Technology, Inc.
|
|
|