circuitnet
Sponsor
Ormet-TLPS

Highly Thermally & Electrically Conductive TLPS via Filing Paste
New filing highlights advanced sintered metal paste enabling faster installation, superior heat dissipation, higher conductivity, and reliable thermal drain performance without long processing cycles.
Ormet TLPS
Air-Vac-Engineering
Sponsor
Master-Bond

Epoxy Offers Ultra High Heat Transfer
Bond EP5TC-80 is a NASA low outgassing rated epoxy that achieves a thermal conductivity of 3.3-3.7 W/(m·K), while also retaining its electrical non-conductivity.
Master Bond

Room Temperature Fast Flow Reworkable Underfill for LGA



Room Temperature Fast Flow Reworkable Underfill for LGA
With the miniaturization of electronics, Land Grid Array has been widely used in consumer electronics, leaving only 20-30 microns gap left between LGA and the substrate.
Technical Paper

DOWNLOAD

Authored By:


Mary Liu, Ph.D., and Wusheng Yin, Ph.D.
YINCAE Advanced Materials, LLC
Albany, NY, USA

Summary


With the miniaturization of electronic device, Land Grid Array (LGA) or QFN has been widely used in consumer electronic products. However there is only 20-30 microns gap left between LGA and the substrate, it is very difficult for capillary underfill to flow into the large LGA component at room temperature. Insufficient underfilling will lead to the loss of quality control and the poor reliability issue.

In order to resolve these issues, a room temperature fast flow reworkable underfill has been successfully developed with excellent flowability. The underfill can flow into 20 microns gap and complete the flow of 15mm distance for about 30 seconds at room temperature. The curing behavior, storage, thermal cycling performance and reworkability will be discussed in details in this paper.

Conclusions


1. Underfill Y can flow fast at room temperature and easily flow into narrow gap of advanced components such as LGA and QFN;

2. Room temperature fast flow underfill is compatible with the flux residue of solder paste;

3. Underfill Y can provide excellent reliability and underfill voids free, high throughput process and also very easy to rework

Initially Published in the SMTA Proceedings

Comments

No comments have been submitted to date.

Submit A Comment


Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Circuit-Technology-Center

6 Common Mistakes of BGA Rework
BGA rework is one of the most challenging procedures you may need to master. Doing it right depends in large part on the skills and knowledge of the rework technician. Learn more ...
Circuit Technology Center