circuitnet
Sponsor
Glenbrook-Technologies

PCB Rework Evolves, With X-ray a Constant Support
Mini Micro Stencil, a contract manufacturer focused on PCB rework, has relied on real-time X-ray inspection to verify its precision rework as the industry has evolved over 30 years.
Glenbrook Technologies
Alltemated
Sponsor
Master-Bond

Epoxy Offers Ultra High Heat Transfer
Bond EP5TC-80 is a NASA low outgassing rated epoxy that achieves a thermal conductivity of 3.3-3.7 W/(m·K), while also retaining its electrical non-conductivity.
Master Bond

UV Conformal Coating Process Development



UV Conformal Coating Process Development
This paper provides a review of a conformal coating process development for a coating using UV light to provide the cure mechanism.
Technical Paper

DOWNLOAD

Authored By:


Corey Peterson
Rockwell Automation
Mequon, WI, USA

Summary


Ultraviolet (UV) curable coatings can be used to meet cost pressures and for improved coating performance when compared to other coating material. However, there are some unique process controls that need to be put in place to guaranty a well controlled process that does not require cleaning. This paper provides a review of a conformal coating process development for a coating using UV light to provide the cure mechanism.

A UV conformal coating line will usually consist of an In-feed conveyor, Coating applicator, Inspection station, UV Oven and an Out-feed conveyor. The UV oven and the coating applicator are the actual components in the line that require an understanding of the process mechanism and the effect that machine settings have on the process

Conclusions


Several factors have been shown to affect coating thickness and a regression equation with good correlation index has been established to fit this model. UV cure parameters require a complete systems view; it is not just conveyor speed but position within the oven as well as fixturing Finally you must understand your incoming board cleanliness and the amount of "process dirt" that the assembly process reduces the surface energy

Initially Published in the SMTA Proceedings

Comments

No comments have been submitted to date.

Submit A Comment


Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Ormet-TLPS

AIT ORMET® TLPS for Thermal Conductivity
AIT ORMET® TLPS is proven with stress relief for stable long-term metallic thermal conductivity & low thermal interface resistance for high temp >175°C
Ormet TLPS