What is an Acceptable Level of Exposed Copper?



What is an Acceptable Level of Exposed Copper?
Is there an acceptable level of exposed copper on gold plated circuit boards where all the conductors are gold plated?
Board Talk
Board Talk is presented by Phil Zarrow and Jim Hall of ITM Consulting.
Process Troubleshooting, Failure Analysis, Process Audits, Process Set-up
CEM Selection/Qualification, SMT Training/Seminars, Legal Disputes
Phil Zarrow
Phil Zarrow
With over 50 years experience in PCB assembly, Phil is one of the leading experts in SMT process failure analysis. He has vast experience in SMT equipment, materials and processes.
Jim Hall
Jim Hall
A Lean Six-Sigma Master Blackbelt, Jim has a wealth of knowledge in soldering, thermal technology, equipment and process basics. He is a pioneer in the science of reflow.

Transcript


Phil
Welcome to Board Talk. We're the Assembly Brothers, Jim Hall and Phil Zarrow of ITM Consulting. Jim, what is today's questions.

Jim 
Phil, this is an anonymous question. We don't even have the initials of the perpetrator of this question. It relates to the surface finishes on printed circuit boards.

The question is: Is there a general specification for an acceptable level of exposed copper for circuit conductors on circuit boards where all the copper surfaces are gold plated? And a further question is: What problems could we see if there are very small non-contact areas on some conductors that have exposed copper?

Phil
Well let's see, the answer to the first question, general specification: YES - generally speaking there shouldn't be any exposed copper. As far as potential problems you could see, well obviously that copper can corrode, discolor.

The thing here is, we would politely say, This a process indicator. It's also a supplier indicator. What kind of crappy boards are you buying? What's with this exposed copper?

Hey, it's supposed to be gold plated, why the hell is the copper showing through here? You know what's going on here? This is a process out of control.

Jim
But let's apply some logic to this, Brother Phil. What is special about gold?

It's expensive.

Jim
So in the fab process that calls for gold coating, obviously any supplier doesn't want to put anymore gold on than they absolutely have to.

Now what happens in real life? Some board fabricators are reasonable about that, they try to keep it low, but well within the specs. Others try to take it right to the limit of the spec.

Phil
And cross over the line.

Jim
So one thing might be here as a process indicator, you might want to measure the average thickness of the gold on the other conductors. Is it not only exposed on little edges and so forth, but is it really thin on the other places so you can't see it, but whereas it might not give you 100% protection? The question I would have is: Are you getting good soldering on all of your joints that are supposedly fully protected by this gold coating?

Phil
And I'd particularly concerned also about the inside barrels of the through-holes and vias. If you're seeing it on the surface, one can only wonder what's beneath. If it's exposed copper, wow, the guys even skipping on the nickel for crying out loud. What is this world coming to, Jim?

Jim
Well remember, we don't know that. There are flash gold finishes that go right over copper, Phil, so we don't know that specifically here. We typically think of a ENIG finish where we get a nickel barrier, and I agree with Phil, but we don't have data here to make that claim.

If it is a ENIG finish and you got exposed copper, then Phil's right; not only did they not get the gold on, but they didn't get the nickel on, which brings us to another thing that you have to ask is: Was it not a problem with the gold being too thin but the fact that the copper wasn't cleaned adequately underneath, and that's death with any finish. Just remember, I don't care what your surface finish is - OSP, immersionsilver, HASL or anything, you're starting with bare copper and you've got to get that copper clean.

All of the surface coating methodologies start by actually etching a little bit of the copper off to get any deep seated corrosion. You get down to really virgin copper. So whatever finish you put on gold or nickel or whatever, you can get a good complete coverage.

Phil
So coming or going, it's a process out of control. This case it could be poor cleaning at one end and/or skimping on the gold at the back end. Nevertheless, it might be time to look for another vendor or get this one in line.

Jim
Yes, unfortunately where so much of the PCB fab is gone offshore, the supply link is longer and problems have increased.



Comments

There were some talks few years back about gold directly over bare copper surface finish. Where soldering will be done directly to copper and the gold is acting as a corrosion resistance. I believe Macdermid was involved with such process. What happened to this finish? Is anyone in the industry using it?
Sherif Refaat, TRCI, Canada
SnCu is being proposed as an alternate to SAC materials because they are cheaper and supposedly process better. Why shouldn't I convert all my SAC PCBA to SnCu if it's so good. There have to be negatives.
Timothy Holder, GE Consumer & Industrial
Did I miss the answer to the question? Is there an acceptable level of exposed copper on flex and rigid boards?
Michael Schulz

Submit A Comment


Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Schunk

What are your economic depaneling needs?
Our depaneling machines are high-performance machines for single circuit boards with electronic components. The cutting principles are fast, the best quality.
SCHUNK