circuitnet
Sponsor
Indium Corporation
High-Reliability for Low-Temp Processes
Durafuse® LT low-temp, high-rel solder paste is bismuth-free, reduces warpage in large BGAs, enhances thermal cycling, drop shock reliability and reduces energy use up to 15%.
Indium Corporation
Openair Plasma for Semiconductor Manufacturing
Sponsor
AI Technology, Inc.
Corrosion, UV Protection for Power Transmission
Moisture, corrosive gas, oxidation & UV blocking prop-erties. FLUOROSEAL® conformal coating for electrical contacts & ceramic insulator protection.
AI Technology, Inc.

Is There a Limit to the Step in a Step Stencil?



Is There a Limit to the Step in a Step Stencil?
I've seen a problem with the 3-mil step. Is there a rule of thumb regarding the amount of step that can used in a step stencil?
Board Talk
Board Talk is presented by Phil Zarrow and Jim Hall of ITM Consulting.
Process Troubleshooting, Failure Analysis, Process Audits, Process Set-up
CEM Selection/Qualification, SMT Training/Seminars, Legal Disputes
Phil Zarrow
Phil Zarrow
With over 50 years experience in PCB assembly, Phil is one of the leading experts in SMT process failure analysis. He has vast experience in SMT equipment, materials and processes.
Jim Hall
Jim Hall
A Lean Six-Sigma Master Blackbelt, Jim has a wealth of knowledge in soldering, thermal technology, equipment and process basics. He is a pioneer in the science of reflow.

Transcript

Phil
Welcome to Board Talk. It's Jim Hall and Phil Zarrow, the Assembly Brothers, who by day go as ITM Consulting. So what is today's question?

Jim
It comes from B.B. The question is about step stencils.

I've used step stencils with one and two mil steps successfully. But recently, I've seen a problem with the 3-mil step. This is an 8-mil foil step down over most of the printed area to a 5 mil thickness.

The problem I am seeing is that the stencil tends to warp around apertures, particularly in areas like fine pitch where there are long apertures close together and the remaining material is a thin strip. The warp makes the stencil act thicker, allows more paste to be deposited leading to bridges on fine pitch QFPs.

Is there a rule of thumb regarding the amount of step that can be etched into the stencil?

Phil
Well, yes there is.  It's been speculated for many, many years. I know back, years ago, we used to use about 2-mil step, but now I think the common wisdom is one about 1.5 mil.

Jim
My experience is that most everybody who does step stencils feels comfortable with the 1-mil step. A lot of people use 1.5 mil. Above that, very few people like to go more than a 1.5 mil to get repeatable printing.

But this raises other questions. This is really a step-up stencil. Where most of the area of the stencil is the lower thickness and you are stepping up for a few thicker areas. I don't know that much about the specifics of the stencil fab, but this seems like a common issue that you should discuss with your stencil manufacturer.

Because if you're getting that problem, you're paying for the stencil and you're probably paying extra get all that extra material etched off or whatever milling process they use to reduce thickness.

Perhaps it's something about the pressure, the squeegee or something that you're using that's causing the stencil to be damaged.

Phil
But either way, 3 mils is really pushing the envelope or in this case, pushing the aperture.

Jim
Although we should say stencil manufacturers have successfully stepped 5, 7, 8 mils, but I honestly have never seen an application. The question - is this a viable robust process to put into a manufacturing operation. So our general rule is 1.5 mils, maybe to 2 mils, but 3 mils definitely goes over rule.

Phil
Well, good, I think we answered that question. Regardless of whatever you are stepping down on your solder paste, when you go to reflow it.

Jim
Don't solder like my brother.

Phil
Hey, don't solder like my brother.

Comments

Dec 1, 2023
One issue I did not see in the discussions is the relationship between height and the transition area. As the height increases the free space surrounding the step needs to increase to absorb the blade distortion. Smoothing the edges at the step can reduce blade wear but may not help with distortion of the blade. There also needs to be enough flat space on the step for a clean wipe. As frequently happens the design often requires smaller parts near your solder hungry part leading to trade offs. Over printing along with a shorter step may also be a solution to add more solder without getting excessive on the step height.

Another potential solution would be to use solder preforms to supplement the solder joint. There are now pick and place feeders that take solder wire and form it into a placeable part. This reduces the cost of a preform making it a viable solution for adding solder.
Don Adams, Bose
Jun 20, 2022
Years ago I worked for a manufacturer of electroformed stencils (I believe the company is now a subsidiary of StenTech). I routinely produced stepped stencils with 0.5-5mil step ups. Most required additional photolithography steps and secondary plating, some I let physics do the work during a single plate-up. If secondary/step phototool alignment is good, the step can be very close to surrounding apertures.
Jeff Marten, Schlage Lock
Jun 10, 2020
Depends on the Step technology we could step up to 20 mils without any issue. Rule of thumb when you are stepping stencils is the clearance between the step island and the aperture openings in the surrounding area. If you are only stepping by few mils, I would recommend Laser Weld technology over any other technology due to surface roughness that created by the chemically etch process. Also, laser weld technology gives you a nice elevation around the island, so that you are not crashing your squeegee too hard.
Prakash, StenTech
Apr 15, 2019
I'd say that Frederick Cox, Metal Etching Technology Associates Inc., is right on the money, when using a isolated step up don't chem etch the rest of the foil, use laser welded inserts, there are several large stencil houses with this technology, and leave room for the squeegee transition, about 50 mils for a 2 mil step up, 75 mils - 100 mils for a 3 mil step up if your design allows for it.
Jim Dowsey, SANMINA
Sep 17, 2018
Depending on your screen printer, you may consider utilizing on-board dispense capability if available. This solution will allow you to utilize a single thickness stencil optimized for the smaller components and supplement areas where additional paste volume is required. These systems are cost effective and, in our case, offer the flexibility of single or dual dispense heads therefore paste and glue can be applied to the same board if necessary. We dispense dots as well as lines for fencing applications.
Mark Brawley, Speedprint Technology
Jun 2, 2016
Years ago I worked with Great Lakes on a process to obtain a tapered stencil. essentially this is a step stencil with incremental steps then polished to obtain the thickness without the harsh edge. For a paste in hole connector, with 16 mil pitch QFNs 4 inches away, this worked well for me.

You do need considerable clearance between any fine pitch and the component that requires the thicker solder, but it can be done, and No, it is not cheap. But if you need it, see what your Stencil house can do, it might surprise you.
Bruce Webster, Iridium Communications
Jun 2, 2016
We laser weld our steps into the foil, as described by Fraser above. Larger steps can be made quite easily. Printing successfully today really depends a lot on your spacing. As long as you have enough space between the large step areas the squeegee blade should be able to transition to the secondary thickness.
Frederick Cox, Metal Etching Technology Associates Inc.
Jun 2, 2016
We have consistently produced stencils with 1 through 10 mil step depths using the appropriate alloy metal. Customers doing two print applications to print fencing often do a 10 mil step. Stencil vendors who are unable to chem-etch the multi-levels are the ones saying you don't need them - or they say they can't be done.
Mark Devereaux, Photo Etch Technology
Jul 15, 2015
We have an application where we go from a 5 mil overall stencil thickness and step up to 12 mils for a transformer (bell shaped pegs for leads). The stencil is etched. There is a 20-mil pitch IC (thus the 5 mil overall stencil thickness). We have had good success with this.
Doug Miller, Miller Electric
Jul 14, 2015
You hit the nail on the head with stencil Fab technology. The truth is that there is tolerance on most step foil fabrication methods. That tolerance can be as much as 20%. Obviously the thicker the step the more effect this has. Tannlin Multi Level doesn't suffer from this as we laser weld inserts into the blank. This means we can deliver 2% thickness control. Since we have introduced this product we have seen step foils get more and more radical as our customers see that we are actually in control of step stencil aperture volumes. Another advantage is that we can ramp up and down to allow the squeegee or the print head a smooth transition. 4mil steps are not uncommon now.
Fraser Shaw, Tannlin
Jul 13, 2015
Best practice is to try avoiding step stencils, there are better technologies in the market like foil types and coating technology which allow releasing more solder volume with the same thickness. This would help when there is a mix of large and small components. But when it's not an option and step is needed, then enlarging the apertures for the bigger parts in order to reduce step thickness to lowest possible would be the best. It's not recommended to work on thickness only and end up with big step thickness.
Labib Saleh, FCT Assembly
Jan 6, 2015
I agree with Jim 3 mils is off the chart, I would look into fab and Gerber to customize opening of apertures to make sure it matches and prevent solder bridges, you never know I've seen a lot of fab that doesn't match up with G editing plays a big part. Skies the limit.
Tuan Nguyen, Radian Smt Technology, USA
Jul 25, 2012
We successfully produce 3 mil step stencils using a special stainless steel alloy. 1 and 2 mil step up and downs are very common - but we do see a 3 mil step once in a while.
Mark, Photo Etch Technology, USA
Jul 25, 2012
With regards to step stencils the warp within the stencil, limits and the print performance depends on the substrate material being used. There are specific materials on the market that are designed to decrease this warp and also generate consistent printing. Datum Fine Grain (FG) is a stainless steel specifically designed to eliminate these issues.
Peter Anniss, Datum Alloys, UK
Submit A Comment
Comments are reviewed prior to posting. You must include your full name to have your comments posted. We will not post your email address.

Your Name


Your Company
Your E-mail


Your Country
Your Comments



Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.

Insert Your Email Address

Sponsor
Advanced Interconnections Corp
Introducing our new Board to Board Connectors
These new Board to Board Connectors feature pitch sizes from 0.50 mm to 1.00 mm with multi-pitch and custom pitch designs available. Designed for long-life applications and robust handling.
Advanced Interconnections Corp
Precision Dispensing Solutions