| Sponsor |
|
Epoxy Offers Ultra High Heat Transfer
Bond EP5TC-80 is a NASA low outgassing rated epoxy that achieves a thermal conductivity of 3.3-3.7 W/(m·K), while also retaining its electrical non-conductivity.
Master Bond
|
|
Jet-Dispensed SMT Adhesives for Durable Printed Electronics
This paper discusses the use of jet-dispensed SMT adhesives for increased durability, lower component cost, and new form factor printed electronics.
Technical Paper
DOWNLOAD
|
Authored By:
Leonard Allison
Engineered Materials Systems, Inc.
100 Innovation Court
Delaware, OH 43015
Summary
Polymer Thick Film (PTF)-based printed electronics (aka Printed Electronics) has improved in durability over the last few decades and is now a proven alternative to copper circuitry. This paper discusses the use of jet-dispensed Surface Mount Technology (SMT) adhesives for increased durability, lower component cost, and new form factor printed electronics. Jet-dispensing enables higher assembly speeds, accurate placement of multiple adhesives, smaller surface mount device (SMD) and Z-axis registration tolerance.
Conclusions
More work is needed to develop robust processing of new form factor substrate for pliable and soft electronic circuitry and electrodes. The challenge lies with handling of the varied new substrate. But the need is popularly recognized, and many material suppliers are committed to delivering better solutions.
Initially Published in the SMTA Proceedings
|
Comments
|
No comments have been submitted to date.
|
|
|
|
Free Newsletter Subscription
Circuitnet is built for professionals who bear the responsibility of looking ahead, imagining the future, and preparing for it.
Insert Your Email Address
|
| Sponsor |
|
Affordable Profiling Excellence
Four channels of precision data capture from the most trusted name in thermal profiling. New and improved V-M.O.L.E.™ 2 is the ideal solution for budget-conscious electronics pros. Learn more here.
ECD
|
|
|