Clean before wave soldering

Is it necessary to clean (using isopropyl alcohol) PCBs before wave soldering?

If it is necessary, then why? If not, then why?

Is there alternative practice for this process?

V. S.

Experts Comments

Cleaning PCB's before wave soldering is certainly not a normal procedure.

The only reason I can think of that would require cleaning is if the boards had been contaminated with some material that required IPA to remove.

Boards should not be handled with bare hands as the oils in the skin can contaminate the solder pads and interfere with the solder process.

Kenneth Kirby
Applications Engineer
Speedline Technologies
Mr. Kirby has been in the electronics manufacturing industry for 18 plus years. Over the years Ken has been in roles such as Equipment and Process trainer, Senior Process Engineer, R&D Application Development Engineer and currently Process Application Engineer.

This would only be required if there were heavy deposits of grease or other contaminates on the PCB. Otherwise the normal cleaning action of the flux will provide the cleaning necessary for the soldering operation.

image
Edward Zamborsky
Regional Sales Manager
OK International Inc.
Mr. Zamborsky serves as one of OK's technology advisers to the Product Development group. Ed has authored articles and papers on topics such as; Low Volume SMT Assembly, Solder Fume Extraction, SMT Rework, BGA Rework, Lead Free Hand Soldering, Lead Free Visual Inspection and Lead Free Array Rework.

In my 20 years of experience in PCB assembly, the only time I have seen companies clean before soldering was in very high-end aerospace and military requirements. And there is some logic to this….

The most corrosive or damaging residues on a PCB are the salts (also called “halites” or “activators”) that are in the fluxes. They make the flux “wetter” and help the soldering materials flow into each other, creating stronger solder joints. But heat increases the rate of corrosion development, and a warm circuit board in a working electronic device can develop dendrites and other corrosive conditions in just weeks or months. So cleaning AFTER soldering should, in theory, remove these residues and provide PCBs with longer operational lives.

But over the years a few companies cleaned before soldering. Their logic was that cleaning was a cheap way to ensure that (a) no contamination was trapped in the solder joints, which would create a weak joint, and (b) no contamination blocked the flow of solder and produced incomplete wetting. After all, there are many other contaminates on circuit boards besides just fluxes: fingerprints contain salts and oils; but also dust, marking inks, Kapton tape residues, and even humidity all are found on the boards and can cause problems. By removing all those residues they increase the chances for perfect soldering and decrease the opportunities for problems.

There’s no doubt that pre-cleaning adds expense to the manufacturing process. So unless you’re building a space probe that’s engineered for cruising through the solar system, in most cases it is an expense that’s hard to justify. My suggestion would be to do a systematic test of 200 boards; clean 100 and don’t clean the others, and see if your QC people can detect any differences.

image
Mike Jones
Vice President
Micro Care
Mr. Jones is an electronics cleaning and stencil printing specialist. Averaging over one hundred days a year on the road, Mike visits SMT production sites and circuit board repair facilities in every corner of the globe, helping engineers and technicians work through the complex trade-offs today's demanding electronics require.

The first objective especially if the PCB assembly is being manufactured using No clean technology is to avoid handling and contamination where ever possible.

Handling contamination will have the potential for two effects

  1. it may cause soldering problems. Finger grease on its own is not likely to cause this if an alcohol based flux is being used since the solvent will dilute the effect of the contamination and there would be no advantage from a pre-clean in solvent like IPA. However, finger marks also carry salts which may affect soldering if contact with the metallisation is long enough and in a humid atmosphere. If this does cause corrosion and affect solderability then pre-cleaning in solvent just before soldering will not reverse the effect anyway.
  2. if there is contamination, it may also be present in areas not contacted by the flux and its solvent. In this case, the marks with their salt content remain available on the PCB and could initiate future electrical reliability problems in service or reduce adhesion and effectiveness of any post-soldering protective coating. A pre-wash in solvent would eliminate this potential hazard.

The user should therefore assess the extent and nature of handling contamination, the probability flux will wet the affected areas and the service environment for the finished assembly. These are of course all subjective criteria which is why avoiding contamination in the first place is the right way to go.

image
Doug Dixon
Global Marketing Director
Henkel Electronics
Mr. Dixon has been in the electronics field for over twenty years and is the Global Marketing Director with the electronics group of Henkel. Prior to joining Henkel, he worked for Raytheon, Camalot Systems, and Universal Instruments.
Additional Comments
No additional comments have been submitted.

Submit a comment - Add to the discussion.

Your Name
Your Email
Company
Country
Comment
  All comments are reviewed prior to posting. We will only post a comment that includes a name and company. You will receive an email if your comments are posted.
 
Home  |  About Us  |  Advertising  |  Advertising Rates  |  Ask the Experts  |  Calendar  |  Contact Us  |  Free Subscription
Industry Forums  |  Exclusives  |  Letters  |  News  |  Press Releases  |  Viewpoint  |  White Papers

Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 22 Parkridge Road, Haverhill, MA 01835 USA
Copyright © 2012 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Semiconductor Packaging News - Semiconductor and advanced packaging news and information.