BGA re-balled with lead free spheres

How can I attach a BGA device with Sn/Pb solder on a lead free pcb? Must the bga be re-balled with lead free spheres? If so what is the reliability?

J.W.

Experts Comments

You have some options, of all which are viable primarily for prototypes or engineering evaluations

(1) Re-ball the BGA package with Pb-free solder balls
- can be fairly reliable but is time consuming and not viable for production volumes. There are folks that provide this service on outsource basis if you have higher volumes
(2) Use a BGA rework station to attach the Pb/Sn packages as a secondary operation - again reasonably reliable but not viable for production volumes
(3) Use mini-stencil to apply low temp solder paste to the PCB (if real-estate permits access). Hand place your Pb/Sn BGA packages using 2DX and reflow as secondary operation at lower temperature (175oC). This is tricky since solder bridging is difficult to avoid.

image
Peter Greenland
VP Sales & Marketing
Pycon Inc.
Mr. Greenland has 20 years electronics industry experience ranging from circuit board design to product support & repair services. Peter has spent the last 4 years at Pycon Inc. supporting customers that require high mix, low volume manufacturing solutions.

We have been placing SnPb spheres on ENIG for as long as there have been BGA packages .. with good success.

Some of the other mixes are dependant upon the specific finish material employed. IMSn, and IMAg have some concerned.

When reballing, be aware the of alloy created where the replacement Sphere contacts the component attachment as well as the board itself. During reballing some of the solder remains with the component where the previous sphere was attached.

image
Mel Parrish
FSO/Director Training Resources
STI Electronics Inc.
Mel Parrish is the FSO and Director of Training Materials Operations, Soldering Technology International (STI), in Madison Alabama. Before coming to the STI, Mel was the Training Manager for the Electronic Manufacturing Productivity Facility (EMPF) and President of Manufacturing Technology Training Center Inc. (MTTC) in Ridgecrest, CA. He remains active in industry trade associations and organizations such as IPC, SMTA, and SME.

First is the Sn/Pb BGA going to be attached with Sn/Pb on to a lead free finished board such as a lead free HASL or immersions silver? If so this is OK. If this is not the case then reliability of a mixed lead and lead free is questionable. Cooling rates are critical these will affect the lead distribution through out the solder connection, slower is generally not desirable as it allows the lead to segregate in the last to section to cool. How long the Sn/Pb is diffused into the lead free all will case variations in the reliability of the components if lead is well diffused and rapid freezing is controlled there is less of an issue with the lead segregating. This leads to a more desirable solder connection however lead in lead free should try to be eliminated.

image
Karl Seelig
Vice President of Technology
AIM
In his 25 years of industry experience, Mr. Seelig has authored over 30 published articles on topics including lead-free assembly, no-clean technology, and process optimization. Karl holds numerous patents, including four for lead-free solder alloys, and was a key developer of no-clean technology.
Additional Comments
No additional comments have been submitted.

Submit a comment - Add to the discussion.

Your Name
Your Email
Company
Country
Comment
  All comments are reviewed prior to posting. We will only post a comment that includes a name and company. You will receive an email if your comments are posted.
 
Home  |  About Us  |  Advertising  |  Advertising Rates  |  Ask the Experts  |  Calendar  |  Contact Us  |  Free Subscription
Industry Forums  |  Exclusives  |  Letters  |  News  |  Press Releases  |  Viewpoint  |  White Papers

Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 22 Parkridge Road, Haverhill, MA 01835 USA
Copyright © 2012 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Semiconductor Packaging News - Semiconductor and advanced packaging news and information.