August 14, 2006
Coating to stop tin whisker growth?

Is there a conformal coating that will stop tin whisker growth?

Doug Hauck

Experts Comments

There is no conformal coating known to stop tin whisker growth.

image
Yun Zhang
R&D Director
Cookson Electronics, Enthone
Ms. Zhang has a PhD in chemistry/electrochemistry. Experiences include AT&T/Lucent Bell Labs, Technic, Cookson Electronics/Enthone. Areas of expertise include: electroplating; Sn whiskers, wafer bumping, Cu post/pillar, Cu redistribution lines and Sn and SnAg bumps.

No, tin whisker growth cannot be stopped with conformal coating. Conformal coating if properly applied will prevent the electrical shorts associated with tin whiskers on the circuit boards.

image
Edward Zamborsky
Regional Sales Manager
OK International Inc.
Mr. Zamborsky serves as one of OK's technology advisers to the Product Development group. Ed has authored articles and papers on topics such as; Low Volume SMT Assembly, Solder Fume Extraction, SMT Rework, BGA Rework, Lead Free Hand Soldering, Lead Free Visual Inspection and Lead Free Array Rework.

Opinions are somewhat mixed, but the general consensus is that some conformal coatings help mitigate tin whisker formation, whilst other coatings have no effect. It seems to be due to the hardness of the coating – the harder the coating, the better it stops tin whisker propagation (probably due to the force required to penetrate the harder coating).

There was an excellent paper published about this very subject by Mr. Thomas Woodrow of Boeing… I have a copy but its 15Mb. If you search the web for Thomas Woodrow, Boeing, Tin Whiskers you'll pretty much find everything you want to know.

I hope of some assistance.

image
Phil Kinner
European Sales Manager
PVA Inc
Phil Kinner is European Sales Manager of PVA, Inc.

There is no conformal coating that will stop a tin whisker from emanating from a tin-plated surface. However, it has been theorized that once the whisker reaches a certain length it will most likely buckle before it punctures the conformal coating on the adjacent lead. Dr. Henning Leidecker has a paper that discusses the calculations in detail.

image
Dr. Craig D. Hillman
CEO & Managing Partner
DfR Solutions
Dr. Hillman's specialties include best practices in Design for Reliability, strategies for transitioning to Pb-free, supplier qualification, passive component technology and printed board failure mechanisms.

Since the announcement of the EU legislation on RoHS and the move of electronics manufactures to a Pb-free process there has been much concern regarding tin whisker growth on Sn-plated components.

Since Sn-plated components are expected to be the primary plating finish many manufacturers (especially those that manufacture high-reliability devices) are concerned about the long term implications of using Sn-plated components.

There have been a few studies that discuss the benefits of minimizing the impact of Sn-whiskers using a coating (H. Leidecker, and J. Kadesch, "Effects of Uralane Conformal Coating on Tin Whisker Growth", Proceedings of IMAPS Nordic, The 37th IMAPS Nordic Annual Conference, pp. 108-116, September, 10-13, 2000 and Thomas A. Woodrow and Eugene A. Ledbury, "Evaluation of Conformal Coatings as a Tin Whisker Mitigation Strategy", IPC/JEDEC 8th International Conference on Lead-Free Electronic Components and Assemblies, San Jose, CA, April 18-20, 2005.).

In the Boeing paper by Woodrow and co-authors they found that Parylene C and Silicones were the most effective at suppressing whisker growth and acrylics were the least effective. Once whiskers did begin to grow, all of the thinner coatings (approx. 1 mil) were penetrated (except the UR/AR Coating) and none of the thicker coatings (3.9 to 6.0 mils) were penetrated.

So coatings can be a mitigation technique, if the correct material is applied as a thick layer. In order to be sure you have the protection required testing should be done on your parts and components.

image
Dr. Brian Toleno
Application Engineering
Henkel Electronics
Dr. Brian Toleno is the Application Engineering Team leader for Henkel Technologies. He is responsible for the technical service and application engineering for Henkel's electronics assembly materials, including solder paste, underfills, PCB protection materials, and underfills.
Additional Comments
Submit a comment - Add to the discussion.

Your Name
Your Email
Company
Country
Comment
  All comments are reviewed prior to posting. We will only post a comment that includes a name and company. You will receive an email if your comments are posted.
Authentication
Please type the number displayed into the box. If you attempt to submit information and receive an error, you may need to refresh the page and insert the information again.
 
Home  |  About Us  |  Advertising  |  Advertising Rates  |  Ask the Experts  |  Calendar  |  Contact Us  |  Free Subscription
Industry Forums  |  Exclusives  |  Letters  |  News  |  Press Releases  |  Viewpoint  |  Webcasts  |  White Papers
We search for industry news so you don't need to. Circuitnet LLC, 22 Parkridge Road, Haverhill, MA 01835 USA
Copyright © 2013 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Semiconductor Packaging News - Semiconductor and advanced packaging news and information.