Hand soldering process for lead-free

What is the right temperature for hand soldering of lead-free solder (Sn,Ag,Cu) composition is 96.5%,3%,.5% respectively?  Please guide me for best hand soldering performance & precautions.

Veerendra Kumar Singh

Experts Comments

Hand soldering with the lead-free alloy SAC305 is most commonly done in the range of 700-750 F. Some have pushed the limit up to about 800 F, but anything beyond 800 F is definitely not recommended as it could induce damage to the assembly.

You will need to carefully select the core flux and flux percent to achieve good soldering results. Most users have found that 2% or 3% flux by weight is required for good performance with lead-free alloys. Finally, it is also advised to monitor the usage of and selection of liquid flux that is being used to assist with the lead-free hand soldering process. Too many users have been attempting to "solve" the slow wetting behavior of lead-free alloys by adding a more aggressive or greater quantity of liquid flux to the operation. The type and amount of flux need to be controlled to be certain of the reliability of the final assembly.

image
Brian Smith
General Manager - Electronic Assembly Americas
DEK
Mr. Smith has been supporting customers in the electronics assembly industry since 1994. His expertise is focused on solder paste printing and reducing soldering defects. He holds a BS in Chemical Engineering and an MBA in Marketing. He has authored several papers in trade magazines and at industry conferences. He is an SMTA Certified Process Engineer.

Hand solder temperature is dependent on the density of the board. Typically a 750F iron tip is a good starting point. Please remember that SAC305 wets half as fast as Sn63. Therefore longer dwell times are needed this may take as long as 3 seconds with an iron as compared to 1.5 seconds with Sn63.

image
Karl Seelig
Vice President of Technology
AIM
In his 25 years of industry experience, Mr. Seelig has authored over 30 published articles on topics including lead-free assembly, no-clean technology, and process optimization. Karl holds numerous patents, including four for lead-free solder alloys, and was a key developer of no-clean technology.
Additional Comments
No additional comments have been submitted.

Submit a comment - Add to the discussion.

Your Name
Your Email
Company
Country
Comment
  All comments are reviewed prior to posting. We will only post a comment that includes a name and company. You will receive an email if your comments are posted.
 
Home  |  About Us  |  Advertising  |  Advertising Rates  |  Ask the Experts  |  Calendar  |  Contact Us  |  Free Subscription
Industry Forums  |  Exclusives  |  Letters  |  News  |  Press Releases  |  Viewpoint  |  White Papers

Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 22 Parkridge Road, Haverhill, MA 01835 USA
Copyright © 2012 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Semiconductor Packaging News - Semiconductor and advanced packaging news and information.