Rogers Corp Announces Introduction of RO4360 6.15 DK Laminates

For Cost-Efficient Power Amplifier Designs

Chandler, AZ –The Advanced Circuit Materials (ACM) Division of Rogers Corporation has introduced RO4360™ laminates, developed for the special requirements of high-frequency amplifier designers. RO4360 laminates feature a dielectric constant of 6.15 and loss of 0.003 @ 2.5GHz. The laminates are based on a ceramic-filled, thermoset resin system reinforced by glass fiber for excellent mechanical stability compared to PTFE woven glass.

RO4360 laminates provide the performance and reliability designers need in a lower total PCB cost solution. Building on the successful legacy of the company’s RO4350B™ laminate materials, the new product features low dissipation factor, generous power-handling capability, and improved thermal conductivity. Environmentally friendly RO4360 laminate materials are RoHS compliant and compatible with standard printed circuit board processing methods. The copper-clad laminates exhibit a high glass transition temperature (Tg) of greater than 280ºC and a low coefficient of thermal expansion (CTE) in the z-axis (30 PPM/ºC) needed for reliable plated through holes (PTHs) in multilayer circuits.

RO4360 laminates allow designers to reduce circuit dimensions in applications where size and cost are critical. They are the best value choice for engineers working on designs including power amplifiers, patch antennas, and other commercial high-frequency applications.

Contact:
Rogers Corporation


http://www.rogerscorp.com/


This page has been viewed 158 times.

More from Rogers Corporation
August 26, 2010 - Corporate News
Rogers to Show Laminate/Prepreg System Solution at Electronics Midwest
Rogers Corporation will be highlighting the benefits of its new 6.15 dielectric-constant RO4360® laminate and RO4460® prepreg system at the ...
Rogers Corporation
July 27, 2010 - Corporate News
Rogers Teams New Ro4460 PREPREG with RO4360 Laminate
Rogers Corporation has developed the perfect match for their popular RO4360™ laminate: RO4460™ prepreg. Both materials feature dielectric ...
Rogers Corporation
May 5, 2010 - Corporate News
Rogers To Show Thermal & Circuit Solutions At IEEE Int'l Microwave Symposium
Rogers Corporation
May 4, 2010 - Corporate News
Rogers 4360 High Frequency Thermoset Material Wins Award
Rogers Corporation
April 27, 2010 - Corporate News
Rogers To Spotlight Practical PCB Solutions At Del Mar Electronics & Design Show
Rogers Corporation
March 31, 2010 - Corporate News
Rogers Corporation to Display Proven PCB Solutions at IPC APEX EXPO
Rogers Corporation will display some of its high-performance materials for electronic printed circuit boards at the upcoming IPC APEX EXPO™ in ...
Rogers Corporation
March 25, 2010 - Corporate News
Rogers Corp Earns Distinguished Designcon 2010 Paper Award
Rogers Corporation
December 9, 2009 - Corporate News
Rogers Introduces Poron Thinstik Soft Seal Foam Material
Rogers Corporation
October 14, 2009 - Corporate News
Rogers Corp. To Showcase Innovative Advanced Materials at Productronica
Rogers Corporation
September 15, 2009 - Corporate News
Rogers Corp Announces Introduction of RO4360 6.15 DK Laminates
Rogers Corporation
August 27, 2009 - Corporate News
Rogers Corp.To Display High Frequency Laminates at IPC Midwest & PCB West Shows
Rogers Corporation
July 24, 2009 - Corporate News
Rogers Corp. New RO4730 Laminates For Light, Low-Loss Antenna Designs
Rogers Corp.
May 13, 2009 - Corporate News
Rogers To Highlight Breakthrough UL Rating, Advanced Thermal Solutions at PCIM
Rogers Corporation
May 12, 2009 - Corporate News
Rogers Introduces Low-Z Axis Material For Airborne Antenna Applications
Rogers Corporation
May 11, 2009 - Corporate News
Rogers to Introduce New Product & Showcase HF Laminates at IEEE MTT-S
Rogers Corporation
May 8, 2009 - Corporate News
Rogers High Performance Foams Division To Highlight 2 Key Products At SAMPE
Rogers Corporation
May 5, 2009 - Corporate News
Rogers Corp Showcases High Frequency Laminates at Del Mar Electronics Show
Rogers Corporation
April 23, 2009 - Corporate News
Rogers Corporation To Showcase High Frequency Laminates at PCB East
Rogers Corporation
April 9, 2009 - Corporate News
Rogers New RT/DUROID Laminates Wins New Product Award
Rogers Corporation
April 8, 2009 - Corporate News
Rogers Introduces RO4000 LoPro Laminates
Rogers Corporation
April 7, 2009 - Corporate News
Rogers To Feature Printed Electronics, Illuminated Advertising Solutions at Printed Electronics
Rogers Corporation
March 30, 2009 - Corporate News
Rogers Corporation To Showcase High Frequency Laminates At CTIA 2009
Rogers Corporation
March 17, 2009 - Corporate News
Rogers Corporation Showcases High Frequency Laminates At IPC APEX EXPO
Rogers Corporation
February 26, 2009 - Corporate News
Rogers To Feature Advanced Circuit Materials At iMAPS Conference & Exhibition
Rogers Corporation
February 25, 2009 - Corporate News
Rogers Corp. to Showcase High Frequency Laminates at Satellite 2009 EXPO
Rogers Corporation

To find more articles from Rogers Corporation, use the search form below.




Home  |  About Us  |  Advertising  |  Advertising Rates  |  Archives  |  Ask the Experts  |  Calendar  |  Circuitmart  |  Corporate News  |  Contact Us
Free Subscription  |  Industry Forums  |  Equipment Mart  |  Exclusives  |  Letters  |  News  |  Site Map  |  Viewpoint  |  White Papers


Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 22 Parkridge Road, Haverhill, MA 01835 USA
Copyright © 2009 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Circuitmart - Video and audio program covering the global electronics assembly marketplace.

Semiconductor Packaging News - Semiconductor and advanced packaging news and information.