Chandler, AZ - Rogers Corporation (NYSE:ROG), a leading supplier of high frequency laminates for decades, will feature several high performance solutions from its family of advanced circuit materials at the 2009 Satellite show, in Washington D.C., March 25-27th (Booth #269)
Rogers Corporation, Advanced Circuit Materials Division, is excited to announce the launch of two new materials especially targeted to meet next generation material requirements for the aerospace and defense industry:
RT/duroid® 5880LZ Laminates
PTFE composites designed for exacting stripline and microstrip circuit applications. Our ground-breaking filler system results in a low density (1.37 gm/cm3), lightweight material for high performance weight sensitive applications. The 1.96 dielectric constant of RT/duroid 5880LZ laminates is among the lowest available for any microwave PCB material. In addition, the dielectric constant is uniform from panel to panel and constant over a wide frequency range. Its low dissipation factor extends the usefulness of RT/duroid 5880LZ to Ku-band and above.
RT/duroid 6202PR High Frequency Materials
RT/duroid 6202PR high frequency circuit material is a low loss and low dielectric constant laminate offering superior electrical and mechanical properties essential in designing complex microwave structures which are electrically stable and used for planar resistor applications. Excellent dimensional stability (0.05 to 0.07 mils/inch) is achieved by the addition of limited woven glass reinforcement. This enables the manufacture of very tight tolerance planar resistors.
In addition, the following well known laminates for high performance satellite applications will be on display:
RT/duroid 5000: Features the lowest electrical loss for reinforced PTFE; uniform electrical properties over frequency; and excellent chemical resistance.
RT/duroid 6000: Features electrical properties; tight DK, thickness control; extremely low TCDK; and low out-gassing, ideal for space applications.
RO3000® High Frequency Laminates: Features low dielectric loss for high frequency applications; uniform mechanical properties, ideal for multi layer board; as well as stable DK versus frequency and temperature.
TMM® material: Features exceptionally low TCDK; a wide range of DK values; and thermoset resin for wire bonding.
RO4000®: Features excellent electrical properties with low DK tolerance and loss; the best overall value for high frequency applications; low thermal coefficient of expansion (CTE) and excellent dimensional stability.
December 9, 2009 - Corporate News
Rogers Introduces Poron Thinstik Soft Seal Foam Material
Rogers Corporation
|
October 14, 2009 - Corporate News
Rogers Corp. To Showcase Innovative Advanced Materials at Productronica
Rogers Corporation
|
September 15, 2009 - Corporate News
Rogers Corp Announces Introduction of RO4360 6.15 DK Laminates
Rogers Corporation
|
August 27, 2009 - Corporate News
Rogers Corp.To Display High Frequency Laminates at IPC Midwest & PCB West Shows
Rogers Corporation
|
July 24, 2009 - Corporate News
Rogers Corp. New RO4730 Laminates For Light, Low-Loss Antenna Designs
Rogers Corp.
|
May 13, 2009 - Corporate News
Rogers To Highlight Breakthrough UL Rating, Advanced Thermal Solutions at PCIM
Rogers Corporation
|
May 12, 2009 - Corporate News
Rogers Introduces Low-Z Axis Material For Airborne Antenna Applications
Rogers Corporation
|
May 11, 2009 - Corporate News
Rogers to Introduce New Product & Showcase HF Laminates at IEEE MTT-S
Rogers Corporation
|
May 8, 2009 - Corporate News
Rogers High Performance Foams Division To Highlight 2 Key Products At SAMPE
Rogers Corporation
|
May 5, 2009 - Corporate News
Rogers Corp Showcases High Frequency Laminates at Del Mar Electronics Show
Rogers Corporation
|
April 23, 2009 - Corporate News
Rogers Corporation To Showcase High Frequency Laminates at PCB East
Rogers Corporation
|
April 9, 2009 - Corporate News
Rogers New RT/DUROID Laminates Wins New Product Award
Rogers Corporation
|
April 8, 2009 - Corporate News
Rogers Introduces RO4000 LoPro Laminates
Rogers Corporation
|
April 7, 2009 - Corporate News
Rogers To Feature Printed Electronics, Illuminated Advertising Solutions at Printed Electronics
Rogers Corporation
|
March 30, 2009 - Corporate News
Rogers Corporation To Showcase High Frequency Laminates At CTIA 2009
Rogers Corporation
|
March 17, 2009 - Corporate News
Rogers Corporation Showcases High Frequency Laminates At IPC APEX EXPO
Rogers Corporation
|
February 26, 2009 - Corporate News
Rogers To Feature Advanced Circuit Materials At iMAPS Conference & Exhibition
Rogers Corporation
|
February 25, 2009 - Corporate News
Rogers Corp. to Showcase High Frequency Laminates at Satellite 2009 EXPO
Rogers Corporation
|
February 10, 2009 - Corporate News
Rogers Issues New Selection Guide for its Bisco Silicone Materials
Rogers Corporation
|
December 10, 2008 - Corporate News
Rogers Corporation Issues Patent Infringement Complaint
Rogers Corporation
|
September 18, 2008 - Corporate News
Rogers Featrues Antenna Grade Materials at Antenna Show
Rogers Corporation
|
September 12, 2008 - Corporate News
Roger's Bisco L3-A Silicone on Track for INNOTRANS
Rogers Corporation
|
May 28, 2008 - Corporate News
IT Will be Rogers' World at MTT-S Atlanta
Rogers Corporation
|
May 14, 2008 - Corporate News
Rogers Corp. Launches Its E/bak™ Cushion Mounting Materials
Rogers Corporation
|
May 6, 2008 - Corporate News
Rogers Corp. Features R/bak SA 3000 Cushion Mounting Tapes
Rogers Corporation
|