Zestron introduces VIGON A 250
Manassas, Va. – ZESTRON America is pleased to introduce its newly developed water-based defluxing agent for spray-in-air processes with low to medium pressure cleaning applications with long exposure times.
VIGON A 250 is an MPC Technology based cleaning agent recommended for removing the latest, most difficult leaded and lead-free flux residues from electronic assemblies in batch cleaning systems as well as in centrifugal and ultrasonic cleaning applications. Its high bath loading capacity ensures extended bath life, low maintenance cost and reduced cost per cleaned part. Due to the surfactant-free formulation, VIGON A 250 eliminates the formation of white residues on cleaned parts and cleaning equipment and it eradicates time-consuming surfactant monitoring.
VIGON A 250 is an aqueous cleaning agent and is therefore biodegradable. It is free of any halogenated compounds and is environmentally friendly. Additionally, the MPC based cleaning agent meets the new RoHS and WEEE guidelines as well as current worker safety standards and actual applicable environmental requirements. Its formulation is free of any other banned hazardous substances.
The newly developed cleaning agent was successfully tested and passed the current electronic manufacturing industry standards such as IPC-610A, J-STD 001D, IPC-TM 650 and J-STD 003.
Contact:
ZESTRON
Sylvain Chamousset
http://www.zestronusa.com
|
This page has been viewed 135 times. |
We search for industry news, so you don't need to.
You would be much better informed if you could read every
important article impacting the electronics assembly and EMS
market. But you can't spend all day searching for them.
Let us do the searching for you.
Get a Free Subscription to Circuitnet
|
|
More from ZESTRON
December 1, 2008 - Corporate News
Cleaning Prior to Conformal Coating - ZESTRON Presented at the Penang SMTA Vendor Day
ZESTRON
|
November 20, 2008 - Corporate News
Stoelting Approves Compatibility with ZESTRON Cleaning Agents
ZESTRON America
|
November 17, 2008 - Corporate News
Flip Chip Cleaning with VIGON® A 201
ZESTRON
|
November 7, 2008 - Corporate News
ZESTRON supports Image Church 5K Race to Benefit MANNA Worldwide
ZESTRON America
|
October 27, 2008 - Corporate News
ZESTRON to Chair the High Performance Electronics Assembly Cleaning Symposium
ZESTRON America
|
October 20, 2008 - Corporate News
ZESTRON to Present and Exhibit at Nutmeg SMTA Vendor Show
ZESTRON America
|
September 29, 2008 - Corporate News
The latest Cleaning and Service Related Trends from Zestron
ZESTRON
|
September 22, 2008 - Corporate News
ZESTRON America to showcase VIGON A 250 at IPC Midwest
ZESTRON America
|
September 10, 2008 - Corporate News
ZESTRON to Exhibit at Arizona-Sonora SMTA Vendor Show
ZESTRON
|
September 8, 2008 - Corporate News
Zestron introduces VIGON A 250
ZESTRON
|
September 3, 2008 - Corporate News
ZESTRON to Present and Exhibit at Capital SMTA Vendor Show
ZESTRON
|
August 5, 2008 - Corporate News
ZESTRON to present 'Fluid Flow Mechanics: New Advances in Low Standoff Cleaning' at the SMTA-I 2008
ZESTRON
|
July 30, 2008 - Corporate News
ZESTRON to Open New Precision Cleaning Center in Ingolstadt, Germany
ZESTRON
|
July 10, 2008 - Corporate News
ZESTRON DS 100: Water-free Defluxing at Low Temperature
ZESTRON
|
June 27, 2008 - Corporate News
Austin American Technology Approves Compatibility with ZESTRON Cleaning Agents
ZESTRON
|
June 20, 2008 - Corporate News
ZESTRON News – The latest Cleaning and Service Related Trends
ZESTRON
|
June 13, 2008 - Corporate News
VIGON SC 200 Reduces Stencil Cleaning Costs by a Factor of 4
Zestron
|
June 9, 2008 - Corporate News
Zestron Selects GEN3 Systems Contaminometer for Ionic Testing
Ascentech
|
June 6, 2008 - Corporate News
ZESTRON America to Exhibit at the Upper Midwest SMTA Expo
ZESTRON
|
May 23, 2008 - Corporate News
ZESTRON America to Showcase "Process Development, Optimization and Cost reduction" at the SMT
ZESTRON
|
May 20, 2008 - Corporate News
ZESTRON America to Announce New North East Sales Manager
ZESTRON
|
May 13, 2008 - Corporate News
ZESTRON further Expands its Asia/Pacific Organization
ZESTRON
|
May 12, 2008 - Corporate News
ZESTRON further Expands its Asia/Pacific Organization
ZESTRON
|
April 30, 2008 - Corporate News
ZESTRON America to Showcase "Complete Cleaning Process Solution" at the 2008 NEPCON East
ZESTRON
|
April 10, 2008 - Corporate News
ZESTRON Asia/Pacific further Expands its Engineering Team
ZESTRON
|
|
|
To find more articles from ZESTRON, use the search form below.
|
|
|
|
|
|
|