WESTMORELAND, N.H. — The leader in harsh environment label materials for product marking and industrial identification, Polyonics Inc., announces that it has been awarded a Global Technology Award in the ID Systems category for its XF-546 Thermal Transfer Printable White Polyimide Label Stock. The award was presented by Global SMT & Packaging Magazine’s Publisher and Editor-in-Chief Trevor Galbraith during a Tuesday, August 19, 2008 ceremony that took place during the SMTA International exhibition and conference in Orlando, FL.
Polyonics XF-546 is a polyimide label material with a permanent, pressure sensitive, silicone adhesive and a high opacity, medium gloss white topcoat specifically designed for thermal transfer printing. The printed polyimide labels withstand long-term temperature exposure as well as higher short-term temperatures (up to 1000°F (538°C)) better than standard polyimides or other high temperature synthetic labels. Surviving temperatures allows XF-546 to work better in today’s changing PCB and component multi pass processing without failing thus eliminating the need for reprinted or replaced labels and increasing manufacturing speeds.
XF-546 is RoHS/REACH compliant and approved for lead-free applications. Each polyimide label produced has excellent resistance to harsh fluxes, cleaners, saponifiers, and wave solder environments, and resists all commonly used methods of cleaning. When matched and printed with the appropriate ribbons XF-546 resists smearing and provides excellent first read rates when scanned.
The Global Technology Awards program is sponsored by Global SMT & Packaging Magazine, and is an annual celebration of product excellence in semiconductor packaging and electronics assembly. Premier products based on the finest examples of creative advancement in technology in key areas are chosen by a distinguished panel of global industry experts.
April 19, 2010 - Corporate News
POLYONICS' TRIBOGARD® Anti-static Label Materials Win a 2010 NPI Award
POLYONICS Inc.
|
November 30, 2009 - Corporate News
Polyonics' Label Materials Receive Approval on Compatibility Testing
Polyonics Inc. announces that its XF-581, XF-582m XF-583, XF-584, XF-596 & XF-597 thermal transfer printable white polyimide label stocks were ...
Polyonics
|
November 13, 2009 - Corporate News
Polyonics' ProductSentry Wins a 2009 Global Technology Award
Polyonics Inc.
|
April 17, 2009 - Corporate News
Polyonics to Debut New Technologies at SMTA Atlanta
Polyonics Inc.
|
April 16, 2009 - Corporate News
Polyonics to Debut New Technologies at SMTA Huntsville
Polyonics Inc.
|
April 15, 2009 - Corporate News
Polyonics Premiers Four New Materials
Polyonics
|
April 2, 2009 - Corporate News
Polyonics’ ProductSentry Wins a 2009 NPI Award
Polyonics Inc.
|
March 25, 2009 - Corporate News
Polyonics to Feature RoHS/WEEE and REACH Compliant Materials at APEX
Polyonics Inc.
|
March 17, 2009 - Corporate News
Polyonics to Host Forum at 2009 APEX Conference & Exhibition
Polyonics Inc.
|
August 27, 2008 - Corporate News
Polyonics' XF-546 Polyimide Label Stock Wins a Global Technology Award
Polyonics
|
August 11, 2008 - Corporate News
Polyonics to Exhibit RoHS/WEEE and REACH Compliant Materials at SMTAI
Polyonics Inc.
|
April 21, 2008 - Corporate News
Polyonics Wins EMAsia Innovation Award for XF-546 Polyimide Label Stock
Polyonics Inc.
|
April 8, 2008 - Corporate News
Polyonics' XF-546 Polyimide Label Stock Wins a 2008 NPI Award
Polyonics
|