Effect on Eutectic Melting point for a multiple alloy board

How do multiple lead-free alloys, combined with a tin-lead Solder Paste, lead-free components, and tin-lead components effect the Eutectic melting points for a solder joint?

As an example: Let's say I am starting with SnPb solder paste and add a few SnPb components with an ENIG (Immersion Gold over Electroless Nickel) circuit card and I add a SnAgCu (Tin, Silver, Copper) alloy BGA. Next, I add some SOICs, QFPs, and PLCCs where the specs identify Tin (lead-free) leads.

This brings ENIG, SnPb, SnAgCu, and possibly 100% Sn all together in one spot, with the common denominator being the SnPb solder paste.

R. S.

This "Ask the Experts" page has been viewed 436 times.

Ask the Experts Comments

July 13, 2008

The simplest answer is that you get a mess.

Consider this; if you take equal amounts of 10/90 tin-lead solder and eutectic 63/37 solder and melt them you end up with 37.5/63.5 solder. The tin-lead binary phase diagram tells us that the liquidus of this composition is 247°C instead of the 183°C we would expect with eutectic solder or the 299°C for 10/90.

Add some SAC with silver, copper and more tin and the resultant mess makes an indistinguishable porridge that defies classification. Given that the eutectic for tin –silver is over 200°C and the addition of more tin to SAC raises the liquidus beyond 217°C, one could assume that you would need higher temperatures to get this porridge to melt and form a joint. But the actual temperature is almost impossible to predict.

The bottom line is don’t mix because you’ll never know for sure what is going on and even worse – if you get it to make an acceptable looking joint there is no knowledge about reliability.

Fred Dimock, Manager, Process technology
BTU International
fdimock@btu.com

Fred DimockMr. Dimock is the manager of Process Technology at BTU International. His extensive experience in thermal processing includes positions at Corning, General Electric, and Sylvania before joining BTU. He has authored numerous articles on lead free processing and process control. He holds Degrees in Mechanical Design and Ceramic Engineering.







Home  |   About Us  |   Advertising  |   Advertising Rates  |   Archives  |   Ask the Experts  |   Calendar  |   Corporate News  |   Contact Us
Free Subscription  |   Industry Forums  |   Equipment Mart  |   Exclusives  |   Letters  |   Circuitmart  |   News  |   Site Map  |   Viewpoint  |   White Papers


Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 135 Ward Hill Avenue, Haverhill, MA 01835 USA
Copyright © 2008 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Visit Semiconductor Packaging News for the latest semiconductor and advanced packaging news and information.