Nihon Superior’s SN100C Wins Two 2008 NPI Industry Awards

OSAKA, JAPAN — Nihon Superior Co. Ltd., an advanced lead-free soldering materials to the global electronics industry announces that it has been awarded two 2008 NPI Awards with the Balver Zinn Balver Zinn Group (Balver Zinn, Nihon Superior Co. Ltd., FCT Assembly and DKL Metals) in the category of Soldering Materials and Flux for its innovative SN100C Paste. The awards were presented to the company during a Monday, March 31, 2008 ceremony that took place in the Mandalay Bay Resort & Convention Center in Las Vegas before the start of APEX 2008.

With its unique tin-copper-nickel-germanium alloy SN100C now firmly established as one of the global electronics industry’s most popular lead-free wave soldering alloys. It has also been found its properties make SN100C an ideal choice for reflow and hand soldering applications.

The fluidity of SN100C, which is comparable to that of tin-lead, is one of the factors that contribute to excellent hole fill and minimal shorts in wave soldering. However, that property is also an advantage in hand soldering where, in combination with the right core flux , it makes possible the completion of more than 35 average joints per minute with a tip temperature of only 380°C. Nihon Superior is now offering the eCore low-spatter lead-free flux-cored solder wire.

The 227°C melting point of SN100C was first thought to preclude its use in reflow soldering but when it was noted that tin-silver-copper alloys (such as SAC305 with a melting point of 217-218°C) are typically reflowed with a peak temperature around 240°C, it was realized that SN100C could be a drop-in replacement. Its high fluidity and excellent wetting properties mean that SN100C can be reflowed successfully at a lower superheat above liquidus than SAC alloys. Nihon Superior now offers SN100C no-clean ePaste for general reflow purposes.

Premiering in 2008, the NPI Awards program is an annual celebration of product excellence in electronics surface mount assembly. Premier products based on the finest examples of creative advancement in technology are chosen by a distinguished panel of industry experts.

Contact:
Nihon Superior Co. Ltd.


http://www.nihonsuperior.co.jp

This page has been viewed 168 times.
We search for industry news, so you don't need to.
You would be much better informed if you could read every
important article impacting the electronics assembly and EMS
market. But you can't spend all day searching for them.


Let us do the searching for you.

Get a Free Subscription to Circuitnet

More from Nihon Superior Co. Ltd.
October 9, 2008 - Corporate News
Nihon Superior to Showcase Newly Expanded Range of SN100C Soldering Materials at Mexitrónica
Nihon Superior
August 27, 2008 - Corporate News
Nihon Superior's New NS-F850 Flux Wins a Global Technology Award
Nihon Superior
August 8, 2008 - Corporate News
Nihon Superior to Display Newly Expanded Range of SN100C® Soldering Materials at Nepcon South China
Nihon Superior
August 7, 2008 - Corporate News
Nihon Superior to Display Complete Range of SN100C products SMTAI
Nihon Superior
May 12, 2008 - Corporate News
Nihon Superior Singapore Celebrates 20th Anniversary
Nihon Superior
May 8, 2008 - Corporate News
Two Industry Names Carry on Family Tradition
Nihon Superior
April 21, 2008 - Corporate News
Nihon Superior Wins a 2008 EMAsia Innovation Award for SN100C
Nihon Superior
April 17, 2008 - Corporate News
Nihon Superior’s SN100C Wins Two 2008 NPI Industry Awards
Nihon Superior Co. Ltd.
April 16, 2008 - Corporate News
Nihon Superior’s SN100C Wins 2008 SMT China Vision Award
Nihon Superior
April 14, 2008 - Corporate News
Nihon Superior Co. Ltd. to Present during International Tin Conference
Nihon Superior Co.
April 9, 2008 - Corporate News
Nihon Superior to attend 18th Shanghai International SMT Conference
Nihon Superior
March 25, 2008 - Corporate News
Nihon Superior Paper on Lead-free Solder Properties at APEX
Nihon Superior
March 24, 2008 - Corporate News
Nihon to Introduce Complete Range of SN100C Soldering Materials at APEX
Nihon Superior
March 14, 2008 - Corporate News
Nihon Superior to Collaborate with University of Queensland
Nihon Superior
March 11, 2008 - Corporate News
Nihon Superior & DfR Solutions’ Lead-free Solder Reliability Paper to be Presented
Nihon Superior
March 11, 2008 - Corporate News
Nihon Superior Impact Strength for BGA Lead-free Solder Spheres Paper
Nihon Superior
February 21, 2008 - Corporate News
Nihon Superior USA to Showcase SN100C at Dallas SMTA Vendor Show
Nihon Superior
February 18, 2008 - Corporate News
Nihon Superior Exhibits SN100C at IPC Int'l Conference on Flexible Circuits
Nihon Superior
February 13, 2008 - Corporate News
Nihon Superior to Introduce Complete Range of SN100C Soldering Materials
Nihon Superior Co., Ltd.
December 19, 2007 - Corporate News
Nihon Superior to Present During the 2008 Pan Pac Symposium
Nihon Superior
To find more articles from Nihon Superior Co. Ltd., use the search form below.





Home  |   About Us  |   Advertising  |   Advertising Rates  |   Archives  |   Ask the Experts  |   Calendar  |   Corporate News  |   Contact Us
Free Subscription  |   Industry Forums  |   Equipment Mart  |   Exclusives  |   Letters  |   Circuitmart  |   News  |   Site Map  |   Viewpoint  |   White Papers


Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 135 Ward Hill Avenue, Haverhill, MA 01835 USA
Copyright © 2008 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Visit Semiconductor Packaging News for the latest semiconductor and advanced packaging news and information.