Coating to stop tin whisker growth?

Is there a conformal coating that will stop tin whisker growth?

Doug Hauck
Amber Waves Elec

This "Ask the Experts" page has been viewed 1582 times.

Ask the Experts Comments

August 16, 2006

Since the announcement of the EU legislation on RoHS and the move of electronics manufactures to a Pb-free process there has been much concern regarding tin whisker growth on Sn-plated components.

Since Sn-plated components are expected to be the primary plating finish many manufacturers (especially those that manufacture high-reliability devices) are concerned about the long term implications of using Sn-plated components.

There have been a few studies that discuss the benefits of minimizing the impact of Sn-whiskers using a coating (H. Leidecker, and J. Kadesch, "Effects of Uralane Conformal Coating on Tin Whisker Growth", Proceedings of IMAPS Nordic, The 37th IMAPS Nordic Annual Conference, pp. 108-116, September, 10-13, 2000 and Thomas A. Woodrow and Eugene A. Ledbury, "Evaluation of Conformal Coatings as a Tin Whisker Mitigation Strategy", IPC/JEDEC 8th International Conference on Lead-Free Electronic Components and Assemblies, San Jose, CA, April 18-20, 2005.).

In the Boeing paper by Woodrow and co-authors they found that Parylene C and Silicones were the most effective at suppressing whisker growth and acrylics were the least effective. Once whiskers did begin to grow, all of the thinner coatings (approx. 1 mil) were penetrated (except the UR/AR Coating) and none of the thicker coatings (3.9 to 6.0 mils) were penetrated.

So coatings can be a mitigation technique, if the correct material is applied as a thick layer. In order to be sure you have the protection required testing should be done on your parts and components.

Dr. Brian Toleno, Application Engineering
Henkel Technologies
brian.toleno@us.henkel.com

Dr. Brian TolenoDr. Brian Toleno is the Application Engineering Team leader for Henkel Technologies. He is responsible for the technical service and application engineering for Henkel's electronics assembly materials, including solder paste, underfills, PCB protection materials, and underfills. He holds a Ph.D. in Analytical Chemistry from The Pennsylvania State University and a B.S. degree in Chemistry from Ursinus College.

August 14, 2006

There is no conformal coating that will stop a tin whisker from emanating from a tin-plated surface. However, it has been theorized that once the whisker reaches a certain length it will most likely buckle before it punctures the conformal coating on the adjacent lead. Dr. Henning Leidecker has a paper that discusses the calculations in detail.

Dr. Craig D. Hillman, CEO & Managing Partner
DfR Solutions
chillman@dfrsolutions.com

Dr. Craig D. HillmanDr. Hillman's specialties include best practices in Design for Reliability, strategies for transitioning to Pb-free, supplier qualification (commodity and engineered products), passive component technology and printed board failure mechanisms. Dr. Hillman has over 30 publications and has presented on a wide variety of reliability issues to over 150 companies and organizations.

August 14, 2006

Opinions are somewhat mixed, but the general consensus is that some conformal coatings help mitigate tin whisker formation, whilst other coatings have no effect. It seems to be due to the hardness of the coating – the harder the coating, the better it stops tin whisker propagation (probably due to the force required to penetrate the harder coating).

There was an excellent paper published about this very subject by Mr. Thomas Woodrow of Boeing… I have a copy but its 15Mb. If you search the web for Thomas Woodrow, Boeing, Tin Whiskers you’ll pretty much find everything you want to know.

I hope of some assistance.

Phil Kinner, Business Director
HumiSeal / Chase Electronic Coatings
PKinner@chasecorp.com

Phil KinnerAs Business Director at HumiSeal, Mr. Kinner oversees all Sales, Marketing, Technical Support and Operational functions within HumiSeal.

August 14, 2006

No, tin whisker growth cannot be stopped with conformal coating. Conformal coating if properly applied will prevent the electrical shorts associated with tin whiskers on the circuit boards.

Edward Zamborsky, Regional Sales Manager
OK International Inc.

Edward ZamborskyMr. Zamborsky serves as one of OK's technology advisors to the Product Development group. Ed has authored many articles, and has presented many papers on topics such as; Low Volume SMT Assembly, Solder Fume Extraction, SMT Rework, BGA Rework, Lead Free Hand Soldering, Lead Free Visual Inspection and Lead Free Array Rework.

August 14, 2006

There is no conformal coating known to stop tin whisker growth.

Yun Zhang, R&D Director
Cookson Electronics, Enthone

Yun ZhangMs. Zhang has a PhD in chemistry/electrochemistry. Experiences include AT&T/Lucent Bell Labs, Technic, Cookson Electronics/Enthone. Areas of expertise include: electroplating; Sn whiskers, wafer bumping, Cu post/pillar, Cu redistribution lines and Sn and SnAg bumps.







Home  |   About Us  |   Advertising  |   Advertising Rates  |   Archives  |   Ask the Experts  |   Calendar  |   Corporate News  |   Contact Us
Free Subscription  |   Industry Forums  |   Equipment Mart  |   Exclusives  |   Letters  |   Circuitmart  |   News  |   Site Map  |   Viewpoint  |   White Papers


Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 135 Ward Hill Avenue, Haverhill, MA 01835 USA
Copyright © 2008 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Visit Semiconductor Packaging News for the latest semiconductor and advanced packaging news and information.