Need lead-free wire solder for hand soldering

We are an EMS company in Israel, We hand solder a lot of lead-free products but yet we have not found an ideal solder wire.  For example: some brands have strong smell, while another produce a lot of smoke.

Can you please recommend an ideal solder wire for Lead-Free based on your experience which is not unpleasant for our employees?

A.N.

This "Ask the Experts" page has been viewed 889 times.

Ask the Experts Comments

September 25, 2006

First of all there should be proper ventilation so that the assembler should not smell the flux. Many fluxes contain acids, amines and resins that can cause irritation to the respiratory system and in some case cause asthma. It is not recommended to breathe any smoke that comes from soldering even in a lead free environment.

There are many good air purification systems that are bench top to eliminate the odor. As far as the solder wire the material with the best SIR, corrosion rating, and that wets is normally the safest for the assembly.

Karl Seelig, Vice President of Technology
AIM
kseelig@aimsolder.com

In his 25 years of industry experience, Mr. Seelig has authored over 30 published articles on topics including lead-free assembly, no-clean technology, and process optimization. Karl holds numerous patents, including four for lead-free solder alloys, and was a key developer of no-clean technology.

September 25, 2006

Beyond the product performance of wetting and low residue, the amount of smoke and type of odor released during soldering is a common concern. Although interconnect performance attributes can be measured objectively, the amount of smoke and smell tend to be more subjective.

Some manufacturers claim to address these concerns as well with specially developed flux cored wire. One such product by Indium Corporation of America (CW-501) is a rosin free no-clean flux cored wire specifically designed to offer superior wetting performance while minimizing smoke and odor. In addition, the flux core is colophony free (does not contain natural pine rosin), which reduces the potential for respiratory issues with operating personnel.

Richard Heimsch, Director
Protean Marketing
rich@proteanmarketing.com

Richard HeimschNow a director at Protean Marketing, Mr. Heimsch has worked in the electronics industry 25+ years in a wide variety of international sales, marketing and operations roles. After spending many yearts in Europe and Asia, Rich now resides in the US where he spearheads Protean's international business development, specializing in Brand Management and Strategic Communications.







Home  |   About Us  |   Advertising  |   Advertising Rates  |   Archives  |   Ask the Experts  |   Calendar  |   Corporate News  |   Contact Us
Free Subscription  |   Industry Forums  |   Equipment Mart  |   Exclusives  |   Letters  |   Circuitmart  |   News  |   Site Map  |   Viewpoint  |   White Papers


Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 135 Ward Hill Avenue, Haverhill, MA 01835 USA
Copyright © 2008 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Visit Semiconductor Packaging News for the latest semiconductor and advanced packaging news and information.