0805 vs. 0603 availability

We have products based on 0805 technology that we are converting to meet the WEEE/RoHS initiative. The concern is having to replace the 0805 with 0603 because of future availability. Should I be concerned in regards to 0805 future availability? If so, what is the time frame?

Roy van Kempen
Honeywell

This "Ask the Experts" page has been viewed 1018 times.

Ask the Experts Comments

November 20, 2006

This question was recently asked by a customer to the SMTA. The following answer was provided by Tom Borkes.

I have not heard this as a definite decision by any of the component manufacturers. However, at best the 0805’s will get more expensive as demand decreases. The 1208 (0.120 in. x 0.080 in. nominal) package that at one time was used en masse has just about gone away (I don’t know, however, if they have stopped making them). The demand for 0805 is following suit, being replaced by still smaller packages (0603, 0402, 0201 and soon, perhaps 01005). The volume demand is from hand-held, wireless products that are constantly reducing size by going to smaller components.

Converting to 0603 for new products is easy (slightly smaller footprint) and probably prudent notwithstanding the suppliers’ plans for the 0805.

Existing designed products are another story. You might want to check directly with the component manufacturers before relaying out the boards.

The 0805 chip capacitors for the most part are exempt from WEEE/RoHS, so I’m not sure the connection there.

Tom Borkes and Joe Belmonte

Joe Belmonte, Project Manager Adv Process Dev
Speedline Technologies
jbelmonte@speedlinetech.com

Joe BelmonteMr. Belmonte has been a process engineer and process engineering manager in the electronic manufacturing industry for over 28 years. Joe is currently a Project Manger at Speedline Technologies Advanced Process Group. Joe's primary responsibilities include managing advanced process development projects such as Lead Free Process Development, and miniature component assembly. Joe has written papers for at numerous industry trade shows and professional society meetings.

November 20, 2006

Good question. Numerous studies have shown 0805 trending towards obsolescence. Of course, by the same token, through hole components went obsolete over 10 year ago.

Obsolescence is primarily an issue for active components, such as microprocessors and memory devices, where the capital costs are so intensive that the business model only makes sense if a very high volume of limited number of technologies is produced. In addition, there is theoretically no downside to going to smaller and smaller feature sizes (excluding reliability, but that’s another topic). This does not apply to ceramic chip capacitors for several reasons.

Number one, and most important, is that smaller margins for passive components make component manufacturers much more receptive to the needs of small volume customers. Number two is that there are downsides to going to smaller components if you need high voltage (most 0603 components are only available in a maximum voltage of 16 or 25V). Number three, there are some passive component manufacturers that specialize in building strictly for the high rel market (as an example, most ceramic caps are still available in a SnPb finish). These buyers will tend to stick with larger case sizes for a some time into the future.

Dr. Craig D. Hillman, CEO & Managing Partner
DfR Solutions
chillman@dfrsolutions.com

Dr. Craig D. HillmanDr. Hillman's specialties include best practices in Design for Reliability, strategies for transitioning to Pb-free, supplier qualification (commodity and engineered products), passive component technology and printed board failure mechanisms. Dr. Hillman has over 30 publications and has presented on a wide variety of reliability issues to over 150 companies and organizations.







Home  |   About Us  |   Advertising  |   Advertising Rates  |   Archives  |   Ask the Experts  |   Calendar  |   Corporate News  |   Contact Us
Free Subscription  |   Industry Forums  |   Equipment Mart  |   Exclusives  |   Letters  |   Circuitmart  |   News  |   Site Map  |   Viewpoint  |   White Papers


Search Category       Search Term   
To search a phrase, place it in quotes.
We search for industry news so you don't need to.

Circuitnet LLC, 135 Ward Hill Avenue, Haverhill, MA 01835 USA
Copyright © 2008 Circuitnet.    All rights reserved.
Jeff Ferry, Publisher  | Ken Cavallaro, Business Manager

Visit Semiconductor Packaging News for the latest semiconductor and advanced packaging news and information.